SEW 092-1990 QSTE500TM HR500F S500MC Pickled Coil Steel Plate 3.0*1250*2500mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of sew 092-1990 qste500tm hr500f s500mc pickled coil steel plate 3.0*1250*2500mm in China. If you're going to wholesale high quality sew 092-1990 qste500tm hr500f s500mc pickled coil steel plate 3.0*1250*2500mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
SEW 092-1990 QSTE500TM HR500F S500MC Pickled Coil Steel Plate 3.0*1250*2500mm
Description
| Width: | 600-2500mm | Technique: | Hot Rolled Pickled |
|---|---|---|---|
| Type: | Steel Plate,Steel Coil | Standard: | ASTM,AISI,JIS,DIN |
| Length: | 1000-12000mm | Special Use: | High-strength Steel Plate,hot Rolled |
| Thickness: | 0.5-100mm | Surface: | Black Painted |
| High Light: |
3mm Hot Rolled Carbon Steel Plate,3mm Hot Rolled Carbon Steel Sheet,DIN Hot Rolled Carbon Steel Plate |
||
SEW 092-1990 QSTE500TM HR500F S500MC Pickled Coil Steel Plate 3.0*1250*2500mm
EW QStE500TM steel plate/sheet High yield strength for cold forming steels
SEW092 QStE500TM steel plate/sheet,SEW092 QStE500TM steel plate/sheet,we can regard QStE500TM steel plate/sheet as high yield strength steels for cold-forming steels.
QStE500TM steel plate is mainly used as high yield strength steels for cold-forming steels.
The SEW092 QStE500TM steel is equivalent to EN S500MC, NFA E490D, UNI FeE490TM and ASTM X70XLK steel grades.
| QStE500TM SEW092 Number:1.0984 | Comparison of steel grades | |
| EN 10149-2 | S500MC | |
| NFA36-231 | E490D | |
| UNI8890 | FeE490TM | |
| ASTM | 070XLK | |
| BS1449 | - | |
QStE500TM steel Chemical Composition
| Grade | C max | Si max | Mn max | P max | S max | AL max | Nb max | V max | Ti max |
| QStE500TM | 0.12 | 0.50 | 1.7 | 0.025 | 0.015 | 0.015 | 0.09 | 0.2 | 0.15 |
QStE500TM steel Mechnical Properties
| Nominal thickness(mm) | - |
| ReH-Minimun yield strength(Mpa) | 500 |
| Nominal thickness(mm) | - |
| Rm-Tensile strength(Mpa) | 550-700 |
| Nominal thickness(mm) | From3 |
| A-Minimum elongation Lo=5,65√So(%) | 14 |
| Nominal thickness(mm) | to3 |
| A-Minimum elongation Lo=Lo=80mm(%) | 12 |
we are QStE500TM steel suppliers ,also can supply QStE550TM steel,QStE600TM steel,QStE690TM steel,please contact us if you need



Hot Tags: sew 092-1990 qste500tm hr500f s500mc pickled coil steel plate 3.0*1250*2500mm, China sew 092-1990 qste500tm hr500f s500mc pickled coil steel plate 3.0*1250*2500mm suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, Corrugated SS Roof Sheet, Stainless Steel 316 316L 316Ti Sheets And Plates, 400 2 4360 Alloy Pipe, SS410 Stainless Steel Plate