ASTM A240 410S Stainless Steel Plate SS410S 06Cr13 X6Cr13 Metal 60mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a240 410s stainless steel plate ss410s 06cr13 x6cr13 metal 60mm in China. If you're going to wholesale high quality astm a240 410s stainless steel plate ss410s 06cr13 x6cr13 metal 60mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM A240 410S Stainless Steel Plate SS410S 06Cr13 X6Cr13 Metal 60mm
Description
| Material: | Stainless Steel 420 | Shape: | Flat Plate |
|---|---|---|---|
| Thickness: | 1.0-60mm | Width: | 100-3000mm |
| Length: | 2000-12000mm | Surface: | 2B NO.4 NO.1 |
| High Light: |
ASTM 410S Stainless Steel Plate,X6Cr13 Stainless Steel Plate,Metal 60mm Stainless Steel Plate |
||
ASTM A240 410S Stainless Steel Plate SS410S 06Cr13 X6Cr13 Metal Plate
410S STAINLESS STEEL ALLOY
UNS: S41008
EN-DIN: 1.4510
410S Stainless Steel Alloy Data Sheet
410S Stainless Steel is a non-hardening modification of Type 410. A small aluminum addition minimizes austenite formation at high temperatures, thereby restricting the alloy's ability to harden. The result is a soft, ductile condition when the material is rapidly cooled from above the critical temperature. This non-hardening characteristic also retards formation of hardening cracks when the steel is welded. The alloy is completely ferritic in the annealed condition.
Nominal Composition
| C: | 0.080 max |
| Mn: | 1.0 max |
| P: | 0.040 max |
| S: | 0.030 max |
| Si: | 1.00 max |
| Cr: | 11.50 – 13.50 |
| Ni: | 0.60 max |
| Ti: | 0.20 max |
| Fe: | BAL |
Physical Properties
At 70°F (At 20°C)
Density
0.280 lb./in³ / (7.73 kg/m³)
Modulus of Elasticity (E)
29.0 x 10³ ksi / (200 x 10³MPa)
Coefficient of Expansion
9.6 x 10-6 microinches/in.-°F (32-212°F) / (17.3 μm/m-°C) (0-100°C)
Electrical Resistivity
23.7 μ ohm.in / (60.0 μ ohm.cm)
Thermal Conductivity
15.6 Btu-in./ft.²hr.-°F (100°C)/ (26.9 W/m-K) (100°C)
Applicable Specifications
ASTM A240
Typical Mechanical Properties – Typical Room Temperature Mechanical Properties
Typical mechanical properties are based on AK source, ASTM A240
Condition
Annealed
Tensile Strength (UTS)
65 ksi (448 MPa)
0.2% YS
40 ksi (276 MPa)
Elongation% in 2" (50.8 mm)
25%
Hardness Rockwell
75 HRBW

Hot Tags: astm a240 410s stainless steel plate ss410s 06cr13 x6cr13 metal 60mm, China astm a240 410s stainless steel plate ss410s 06cr13 x6cr13 metal 60mm suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 431 10mm Stainless Steel Plate, Corrugated SS Roof Sheet, SS431 Stainless Steel Plate