S355J2+N Carbon Steel Plates
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of s355j2+n carbon steel plates in China. If you're going to wholesale high quality s355j2+n carbon steel plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
S355J2+N Carbon Steel Plates are light and durable and are more efficient in product and structure. S355J2+N Carbon Steel Plates are made of carbon steel. The alloys used to make these plates have many different properties and characteristics. The alloy used in S355J2+N Carbon Steel plates has a low melting point, so it can also be cold-formed and hot-formed.

| Grade | DIN | ASTM | EN | JIS | Material no. |
|---|---|---|---|---|---|
| S355 J2+N | 17100 St52-3N |
A572-50 | 10025-2:2004 | G3106 SM490YB |
1.0577+N |
| Grade | C | Si | Mn | S | P | C.E |
|---|---|---|---|---|---|---|
| S355 J2+N | 0.22 max | 0.55 max | 1.60 max | 0.035 max | 0.035 max | 0.047 max |
This alloy made of carbon steel leads to form a fragile layer on its upper side to withstand the effects of temperature without any problem. Therefore, they have higher temperature stability and higher heat resistance. Unlike the other steels, besides having a more fragile structure, the carbon steel plates have high tensile strength and elongation and can withstand stress corrosion and cracking. These steel plates also have greater shear strength.

S355J2 N is the type of alloy with great attributes and working properties; hence the plates manufactured using these grades are welder friendly, high tensile strength and low carbon structural steel. These can be readily available to customers in the weldable form. S355J2+N Carbon Steel Plates has excellent cold-forming properties, and plates are often produced using the killed steel process and exported to customers in controlled rolling or normalized conditions.
Hot Tags: s355j2+n carbon steel plates, China s355j2+n carbon steel plates suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Corrugated SS Roof Sheet, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS431 Stainless Steel Plate