EN 10025-2 S355J2G3 High Strength Low Alloy Structural Steel Plate S355j2g3+N
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of en 10025-2 s355j2g3 high strength low alloy structural steel plate s355j2g3+n in China. If you're going to wholesale high quality en 10025-2 s355j2g3 high strength low alloy structural steel plate s355j2g3+n made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
EN 10025-2 S355J2G3 High Strength Low Alloy Structural Steel Plate S355j2g3+N
Description
| Certification: | CE, ISO, BV, SGS | Commodity: | New Product Corten Plate S355-JOWP |
|---|---|---|---|
| Type: | Plate | Material: | S355-JOWP, S355-J2WP |
| Standard: | ASTM, AISI, GB, JIS, EN, DIN | Length: | 1000mm-6000mm |
| Width: | 1000mm-2000mm | Thickness: | 3mm-35mm |
| Technique: | Cold Rolled | ||
| High Light: |
shipping plate,marine steel plate |
||
Professional Ship Steel Plate / 20mm Thick Marine Grade Steel Plate
Quick info:
factory price corten steel plates
>> Length: 1000mm-6000mm
>> Width: 1000mm-2000mm
>> Thickness: 2mm-30mm
>> Standard: AISI, ASTM, JIS, EN, DIN, GB
>> Certification: CE, ISO, BV, SGS

| Commodity | New product corten plate S355-JOWP weathering steel plate at professional design |
| Material | S355-JOWP, S355-J2WP |
| Type | plates, coil, tube |
| Advantage | Rust-resistant, corrosion-resistant life extension, thinning saving, labor saving |
| Application | Container, rolling stock, oil derrick, harbor construction, chemical and petroleum oil platform equipment |
| Stock | always in good stock |
| C | Si | Mn | S | P | Cu | AI | |
| Chemical composition | 0.12-0.21 | 0.2-2.0 | 0.7-2.0 | ≤0.036 | ≤0.034 | 0.1-0.4 | <0.2 |
Corten plates S355-JOWP:
Weathering steel, low-alloy steel is between series, weathering steel and stainless steel to add between ordinary carbon steel by a small amount of copper, nickel and other elements made of corrosion-resistant, high-quality steel with a tough, plastic casting, forming, welding and cutting , abrasion, high temperature, anti-fatigue properties; weather resistance of carbon steel of 2 to 8 times, coating of carbon steel is 1.5 to 10 times.



Packaging & Delivery time
Part 1.
We wrap the corten plates in standard seaworthy packaging by waterproof paper + plywood pallets or as your order quantity.
Part 2.
Delivery time within one week if the quantity less than 100 tons.

Company service:
1.Sample:Free samples will be available for most of the products, but usually the freight ,charges need to paid by your side.
2.Inquiry:24 hours online to ensure your inquiry will be replied within 12 hours .
3.Delivery:Most products can be delivered within 7 days after order.
4.Small order also can be accepted.
RFQ
A: How to make sure the quality of the products?
B: The products is all produced by famous manufactory in China, the quality is good, we can provide the Mill Test Certifiated to the customer. We also acceplt do the SGS quality test before the shipment.
A: What's your deliver times?
B: The deliver time is usually 5-10 days, for the un-standard size products or large quantity, goods, the deliver time will be 15-30 days.
A: Can I get the sample
B: We will provide samples for your testing and inspection for FREE. You only need to pay for the shipping and handling charges.
A:How will you ship our order?
B: Our city is near the Shanghai Port, we will start the shipment at the Shanghai Port. We have our own shiping agent in Shanghai, It's very fast and convinced.
Hot Tags: en 10025-2 s355j2g3 high strength low alloy structural steel plate s355j2g3+n, China en 10025-2 s355j2g3 high strength low alloy structural steel plate s355j2g3+n suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS410 Stainless Steel Plate, SS431 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, Corrugated SS Roof Sheet
You Might Also Like
Send Inquiry