Cold Rolled 2.0mm Seamless Carbon Flat Steel Plate Automotive Steel Sheet
video

Cold Rolled 2.0mm Seamless Carbon Flat Steel Plate Automotive Steel Sheet

SEW QStE500TM steel plate/sheet High yield strength for cold forming steels SEW092 QStE500TM steel plate/sheet,SEW092 QStE500TM steel plate/sheet,we can regard QStE500TM steel plate/sheet as high yield strength steels for cold-forming steels. QStE500TM steel plate is mainly used as high yield strength steels for cold-forming steels. The SEW092 QStE500TM steel is equivalent to EN S500MC, NFA E490D, UNI FeE490TM and ASTM X70XLK steel grades.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of cold rolled 2.0mm seamless carbon flat steel plate automotive steel sheet in China. If you're going to wholesale high quality cold rolled 2.0mm seamless carbon flat steel plate automotive steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Cold Rolled 2.0mm Seamless Carbon Flat Steel Plate Automotive Steel Sheet

Description

Width: 600-2500mm Grade: S500MC
Application: Container Plate Technique: Hot Rolled,Cold Rolled
Type: Steel Plate Standard: ASTM,AISI,JIS,DIN
Length: 1000-12000mm Surface Treatment: Black,hot Finished
Special Use: High-strength Steel Plate Thickness: 2.0-60mm
Shape: Flat Steel Plate
High Light:

seamless Carbon Flat Steel Plate

,

2.0mm Carbon Automotive Steel Sheet

,

Cold Rolled Seamless carbon Steel plate

Grade : S500MC
Number: 1.0984
Classification: Steel
Standard:
EN 10149-2: 1996 Specification for hot-rolled flat products made of high yield strength steels for cold forming. Delivery conditions for thermomechanically rolled steels
Equivalent grades:  

Chemical composition % of steel S500MC (1.0984): EN 10149-2-1996

The sum of Nb, V and Ti shall be max 0.22 %
If agreed at the time of the enquiry and order the sulfur content shall be max 0.01 % (ladle analysis)

 

 

 

C Si Mn P S V Nb Ti Al
max 0.12 max 0.5 max 1.7 max 0.025 max 0.015 max 0.2 max 0.09 max 0.15 min 0.015


New opportunities for buyers!
Post free buying requirement of steel S500MC (1.0984)



Mechanical properties of steel S500MC (1.0984)

Rm - Tensile strength (MPa) 550-700
ReH - Minimum yield strength (MPa) 500
Nominal thickness (mm): to 3
A - Min. elongation Lo = 80 mm (%) 12
Nominal thickness (mm): from 3
A - Min. elongation Lo = 5,65 √ So (%) 14



Equivalent grades of steel S500MC (1.0984)

Warning! Only for reference

EU
EN
USA
-
Germany
DIN,WNr
France
AFNOR
Italy
UNI
Sweden
SS
Inter
ISO
S500MC
Gr.70
E490D
QStE500TM
E490D
FeE490TM
2662
FeE490

Cold Rolled 2.0mm Seamless Carbon Flat Steel Plate Automotive Steel Sheet 0Cold Rolled 2.0mm Seamless Carbon Flat Steel Plate Automotive Steel Sheet 1Cold Rolled 2.0mm Seamless Carbon Flat Steel Plate Automotive Steel Sheet 2

Hot Tags: cold rolled 2.0mm seamless carbon flat steel plate automotive steel sheet, China cold rolled 2.0mm seamless carbon flat steel plate automotive steel sheet suppliers, Corrugated SS Roof Sheet, SS431 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates

Send Inquiry

whatsapp

Phone

E-mail

Inquiry