1.4418 1.4512 Stainless Steel Patterned Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4418 1.4512 stainless steel patterned plate in China. If you're going to wholesale high quality 1.4418 1.4512 stainless steel patterned plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Products Description
1.4418 1.4512 stainless steel patterned plate
Because of preheat threatment, the mechanical properties of this material is very good and also surface hardness is about 30 HRC. So in many applications, no extra heat threatment is necessary. But if necessary, a second heat threatment can be applied to the 1.4418 material and after another heat threatment, the mechanical values can be better. 1.4418 stainless steel equivalent is asked to much to our company but not all the stainless steel grade has an equivalent in AISI norm. So 1.4418 grade do not have any stainless steel grade name like 304 grade or 316 grade. 1.4418 or X4CrNiMo16-5-1 are this grades only names according to EN norm.
Products Properties
Chemical Composition
| Chemical Element | % Present |
|---|---|
| Carbon (C) | 0.0 - 0.30 |
| Chromium (Cr) | 10.50 - 12.50 |
| Manganese (Mn) | 0.0 - 1.00 |
| Titanium (Ti) | 0.0 - 0.65 |
| Silicon (Si) | 0.0 - 1.00 |
| Phosphorous (P) | 0.0 - 0.04 |
| Sulphur (S) | 0.0 - 0.02 |
| Iron (Fe) | Balance |
Properties
| Physical Property | Value |
|---|---|
| Density | 7.6 g/cm³ |
| Modulus of Elasticity | 208 GPa |
| Thermal Conductivity | 25.8 W/m.K |
| Electrical Resistivity | 0.6 x10^-6 Ω .m |
1.4418 1.4512 stainless steel patterned plate

1.4418 grade material has a good corrosion resistance and many people can compare this grade with 630 (1.4542) grade stainless steel. 1.4418 stainless steel usually heat threated in two different heat threatment conditions after production. These heat threatment conditions are QT780 and QT900. All 1.4418 material comes to Bircelik as ,n QT900 (Quenched and Tempered 900) heat threatment condition. So the minimum tensile strenght of the materials at Bircelik warehouse are minimum 900 MPA.
Material 1.4512 / AISI 409 is a rust-resistant ferritic chromium steel. Due to its titanium content, the material is more resistant to corrosion than the ferritic steel 1.4003, but the corrosion resistance is lower than in austenitic stainless steels. Compared to these, however, stainless steel 1.4512 / AISI 409 has a better resistance to stress corrosion cracking. The material is suitable for cold forming and is used, among other industries, in the automotive industry or in mechanical engineering.
Customer Case

FAQ
Q:How do you make our business long-term and good relationship?
A:We keep good quality and competitive price to ensure our customers benefit ; We respect every customer as our friend and we sincerely do business and make friends with them. No matter where they come from.
Q:what is your delivery time ?
A: Our delivery time is about one week, timing according to the number of customers.
Q: How long is your delivery time?
A: It is according to quantity. Generally it is 30 days.
Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight.
Q: What is your terms of payment ?
A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Hot Tags: 1.4418 1.4512 stainless steel patterned plate, China 1.4418 1.4512 stainless steel patterned plate suppliers, SS409 Stainless Steel Welded Pipe, 1 4510 Stainless Steel Patterned Plate, SS410 Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS431 Stainless Steel Plate