ASTM 131 Ship Steel Plate Grade AH36 DH 36 EH36 EH40 9144mmL X 2438mmW X 20mmT
video

ASTM 131 Ship Steel Plate Grade AH36 DH 36 EH36 EH40 9144mmL X 2438mmW X 20mmT

Our steel plates with high wear resistance and good impact performance is good, can be cutting, bending, welding, etc., can adopt welding, plug welding, bolt connection way to connect with other structures, such as the scene of the maintenance process possesses the characteristics of time saving, convenient and widely used in peteoleum, chemical industry, container, shipbuilding, coal, cement, power station, mining, building materials, compared with other materials, has a high cost performance, has been favored by more and more buyers.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm 131 ship steel plate grade ah36 dh 36 eh36 eh40 9144mml x 2438mmw x 20mmt in China. If you're going to wholesale high quality astm 131 ship steel plate grade ah36 dh 36 eh36 eh40 9144mml x 2438mmw x 20mmt made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM 131 Ship Steel Plate Grade AH36 DH 36 EH36 EH40 9144mmL X 2438mmW X 20mmT

Description

Grade: AH36 DH 36 EH36 EH40 Width: 1500-2500mm
Length: 2000-12000mm Thickness: 3-150mm
Use: Shipping Building
High Light:

ASTM 131 Ship Steel Plate

,

Grade AH36 Ship Steel Plate

,

20mm Shipbuilding Steel Plate

ASTM 131 Grade AH36 DH 36 EH36 EH40 High Strength Shipping Steel Plate SIZE : 9144mmL x 2438mmW x 20mmT

Due to the harsh working environment of the ship, the hull shell is subject to chemical corrosion of seawater, electrochemical corrosion and corrosion of marine organisms and microorganisms; the hull is subjected to large wind and wave impacts and alternating loads; the shape of the ship is complicated by processing methods, etc. Steel for hull structure is strictly required. First of all, good toughness is the most critical requirement. In addition, high strength, good corrosion resistance, weldability, forming properties and surface quality are required.
Shipbuilding Steels Our hot rolled shipbuilding steel is produced in accordance with the relevant Classification Society, examples of which include Lloyds Register and Det Norske Veritas.
Our steel products include steel shipbuilding plate, fabricated steel sections and floor plate for decking. We can also supply bulb flats for plate stiffening, structural steel angles and inverted angles.
Our plates are supplied under the ASTM/ASME specification (ASTM A131 / ASME SA 131) which is the standard specification for Structural Steel for Ships. We offer higher strength shipbuilding steels as standard .High strength steels offer significant cost advantages by reducing the weight of the structure in comparison to the steel used.
The plates are suitable for use in the construction of container ships and large cargo freighters as well as commercial shipping lines such as luxury cruise ships and ferries. Supply options include heavy plates, surface treated plates and pre-fabricated sections. In most cases, the steel can also be supplied as hot rolled coils or cut into lengths (sheets).
These high yield materials are commonly used in the construction of hulls and superstructures for large shipping vessels. The grades are exclusively for shipbuilding use as set out in the standard.

Normal steel grade: A B D E
High strength steel grade: A32 D32 E32 F32 A36 D36 E36 F36
Ultra High strength steel grade: AH40 DH40 EH40 FH40
Marine and offshore vessel used steel plate: NV360 NV410 NV460 NV490 NV510 LR360/360FG LR410/410FG LR460FG/490FG/510FG
Classification society: (ASTM A-131)ABS CCS LR VL(GL/DNV) RINA BV NK KR RS IRS VR

Product Specification

Product Name Ship Building Steel Plate
Standard AISI, ASTM, DIN, JIS, GB, SUS, EN, etc.
Material A/B/D/E, A32/D32/E32/F32, A36/D36/E36/F36, A40/D40/E40/F40, A131A/B/D/E/AH32/DH32/EH32, AH36/DH36/EH36, AH40/DH40/EH40, NVA420/D420/E420, NVA460/D460/E460, NVA500/D500/E500, NVA550/D550/E550, NVA, NVD, 16MnL, Q235, Q235B, CCS-A, CCS-B, CCSA, CCSB, CCS, CCSD, CCSE, GL-B, GL-D, GL-E
Length 1000mm-12000mm or as required
Width 600mm-3000mm or as required
Thickness 3mm-300mm or as required
Technique Hot rolled
Surface Treatment Clean, blasting and painting according to customer requirement
Thickness tolerance ±0.15mm
Application To prevent the hull from being corroded by chemical corrosion, electrochemical corrosion and sea life and microorganisms.It is used in make ship body ,decks etc.
MOQ 25tons.We also can accept sample order.
Shipment time Within 15-20 workdays after receiving deposit or L/C
Export packing Waterproof paper, and steel strip packed.
Standard Export Seaworthy Package.Suit for all kinds of transport,or as required
Capacity 250,000 tons/year


Application
Our steel plates with high wear resistance and good impact performance is good, can be cutting, bending, welding, etc., can adopt welding, plug welding, bolt connection way to connect with other structures, such as the scene of the maintenance process possesses the characteristics of time saving, convenient and widely used in peteoleum, chemical industry, container, shipbuilding, coal, cement, power station, mining, building materials, compared with other materials, has a high cost performance, has been favored by more and more buyers.
Factory Wholesale ABS BV CCS Dnv High Quality Shipbuilding Marine Steel Plate Ah32 Dh32 Eh32 Ah36 Dh36 Eh36 Hot Rolled Ship Building Carbon Steel Plate
Chemical Composition

Grade C max Si max Mn P max S max Als min
A 0.21 0.50 ≥ 2.5C 0.035 0.035 -
B 0.21 0.35 0.80-1.20 0.035 0.035 -
D 0.21 0.35 0.60-1.20 0.030 0.030 0.015
E 0.18 0.35 0.70-1.20 0.025 0.025 0.015
Grade C Si Mn P S Als Ti Cu Cr Ni Mo Nb V
AH32 ≤0.18 ≤0.50 0.9~1.6 ≤0.035 ≤0.035 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.40 ≤0.08 0.02~0.05 0.05~0.10
DH32 ≤0.18 ≤0.50 0.9~1.6 ≤0.035 ≤0.035 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.40 ≤0.08 0.02~0.05 0.05~0.10
EH32 ≤0.18 ≤0.50 0.9~1.6 ≤0.035 ≤0.035 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.40 ≤0.08 0.02~0.05 0.05~0.10
FH32 ≤0.16 0.1~0.5 0.9~1.6 ≤0.025 ≤0.025 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.80 ≤0.08 0.02~0.05 0.05~0.10
AH36 ≤0.18 ≤0.50 0.9~1.6 ≤0.035 ≤0.035 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.40 ≤0.08 0.02~0.05 0.05~0.10
DH36 ≤0.18 ≤0.50 0.9~1.6 ≤0.035 ≤0.035 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.40 ≤0.08 0.02~0.05 0.05~0.10
EH36 ≤0.18 ≤0.50 0.9~1.6 ≤0.035 ≤0.035 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.40 ≤0.08 0.02~0.05 0.05~0.10
FH36 ≤0.16 0.1~0.5 0.9~1.6 ≤0.025 ≤0.025 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.80 ≤0.08 0.02~0.05 0.05~0.10
AH40 ≤0.18 ≤0.50 0.9~1.6 ≤0.035 ≤0.035 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.40 ≤0.08 0.02~0.05 0.05~0.10
DH40 ≤0.18 ≤0.50 0.9~1.6 ≤0.035 ≤0.035 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.40 ≤0.08 0.02~0.05 0.05~0.10
EH40 ≤0.18 ≤0.50 0.9~1.6 ≤0.035 ≤0.035 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.40 ≤0.08 0.02~0.05 0.05~0.10
FH40 ≤0.16 0.1~0.5 0.9~1.6 ≤0.025 ≤0.025 ≥0.015 ≤0.02 ≤0.35 ≤0.20 ≤0.80 ≤0.08 0.02~0.05 0.05~0.10


Mechanical Properties

Grade Thickness(mm) max Yieldpoint(Mpa) min Tensile Strength
(Mpa)
Elongation(%)
min
V-impact test cold bend test
Temperature
(ºC)
Average AKV b=2a 180° b=5a 120°
lengthways Min crosswise Min
A 50 235 400~520 22 - - - - d=2a
B 50 235 400~520 22 0 27 20 - d=3a
D 50 235 400~520 22 -10 27 20 - d=3a
E 50 235 400~520 22 -40 27 20 - d=3a
AH32 50 315 440~570 22 0 31 22 - d=3a
DH32 50 315 440~570 22 -20 31 22 - d=3a
EH32 50 315 440~570 22 -40 31 22 - d=3a
FH32 50 315 440~570 22 -60 31 22 - d=3a
AH36 50 355 490~620 21 0 34 24 - d=3a
DH36 50 355 490~620 21 -20 34 24 - d=3a
EH36 50 355 490~620 21 -40 34 24 - d=3a
FH36 50 355 490~620 21 -60 34 24 - d=3a
AH40 50 390 510~660 20 0 41 27 - -
DH40 50 390 510~660 20 -20 41 27 - -
EH40 50 390 510~660 20 -40 41 27 - -
FH40 50 390 510~660 20 -60 41 27 - -

Factory Wholesale ABS BV CCS Dnv High Quality Shipbuilding Marine Steel Plate Ah32 Dh32 Eh32 Ah36 Dh36 Eh36 Hot Rolled Ship Building Carbon Steel Plate

Factory Wholesale ABS BV CCS Dnv High Quality Shipbuilding Marine Steel Plate Ah32 Dh32 Eh32 Ah36 Dh36 Eh36 Hot Rolled Ship Building Carbon Steel Plate

Factory Wholesale ABS BV CCS Dnv High Quality Shipbuilding Marine Steel Plate Ah32 Dh32 Eh32 Ah36 Dh36 Eh36 Hot Rolled Ship Building Carbon Steel Plate


Shipbuilding Plate Available Dimensions

Item Thickness (mm) Width (mm) Length/coil diameter(mm)
Shipbuilding plate 6~50 1300~3000 3000~15000
Shipbuilding coil 6~20 1500~2000 760+20~760-70


Shipbuilding Steel Theoretical Weight

Thickness (mm) Estimate Weight Thickness (mm) Estimate Weight
Kg/ft2 Kg/m2 Kg/ft2 Kg/m2
6 4.376 47.1 25 18.962 196.25
7 5.105 54.95 26 20.42 204.1
8 5.834 62.8 28 21.879 219.8
10 7.293 78.5 30 23.337 235.5
11 8.751 86.35 32 25.525 251.2
12 10.21 94.2 34 26.254 266.9
14 10.939 109.9 35 27.713 274.75
16 11.669 125.6 40 29.172 314
18 13.127 141.3 45 32.818 353.25
20 14.586 157 48 35.006 376.8
22 16.044 172.7 50 36.464 392.5
24 18.232 188.4 - - -

Product Advantage
1.Resistant to wear and crack
Wear protection, scalable, excellent chemical resistance, good alkali-resistant metal and acid energy
2.High toughness
The elongation is required to be 15%~20% and the impact toughness at room temperature is more than 600KJ/M~800KJ/M. For large welded members, high fracture toughness is also required.
3.Advanced technology
The surface carburized layer hardness is high, to ensure excellent wear resistance and contact fatigue resistance, and has the appropriate plasticity and toughness.

Product Display

We can produce different sizes, thicknesses, widths and materials according to your requirements

 

 

ASTM 131 Ship Steel Plate Grade AH36 DH 36 EH36 EH40 9144mmL X 2438mmW X 20mmT 4ASTM 131 Ship Steel Plate Grade AH36 DH 36 EH36 EH40 9144mmL X 2438mmW X 20mmT 5

Hot Tags: astm 131 ship steel plate grade ah36 dh 36 eh36 eh40 9144mml x 2438mmw x 20mmt, China astm 131 ship steel plate grade ah36 dh 36 eh36 eh40 9144mml x 2438mmw x 20mmt suppliers, SS409 Stainless Steel Welded Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, 400 2 4360 Alloy Pipe, SS410 Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry