AH36 A36 HT Steel Plate SIZE: 10 MM THK X 2000 MM X 6000 MM ) OF MIN YIELD STRESS 355N/mm2
video

AH36 A36 HT Steel Plate SIZE: 10 MM THK X 2000 MM X 6000 MM ) OF MIN YIELD STRESS 355N/mm2

ASTM A131 AH36 steel plate, AH36 steel is a kind of steel for shipbuilding and platform. Shipbuilding steel plate AH36 is the high tensile strength steel. As a professional AH36 shipbuilding steel plate exporter, Bebon international can supply steel plate AH36. ASTM A 131 AH36 shipbuilding steel plates can be used in the manufacture of the ship's hull structure whose weight is below 10000 tons.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ah36 a36 ht steel plate size: 10 mm thk x 2000 mm x 6000 mm ) of min yield stress 355n/mm2 in China. If you're going to wholesale high quality ah36 a36 ht steel plate size: 10 mm thk x 2000 mm x 6000 mm ) of min yield stress 355n/mm2 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

AH36 A36 HT Steel Plate SIZE: 10 MM THK X 2000 MM X 6000 MM ) OF MIN YIELD STRESS 355N/mm2

Description

Width: 100mm-3500mm Length: 200-12000mm
Thickness: 1.5-30 Mm Or Customized Grade: AH36 DH36 EH36
Condition: Hot Rolled Use: Shipbuilding

ASTM A131 AH36 steel plate, AH36 steel is a kind of steel for shipbuilding and platform. Shipbuilding steel plate AH36 is the high tensile strength steel. As a professional AH36 shipbuilding steel plate exporter, Bebon international can supply steel plate AH36. ASTM A 131 AH36 shipbuilding steel plates can be used in the manufacture of the ship's hull structure whose weight is below 10000 tons.

AH36 shipbuilding steel plate specification:
Thickness: 4mm to 260mm,
Width: 1200mm to 4000mm
Length: 3000mm to 18000mm.

AH36 steel Chemical Composition %:


Grade

C

max

Si

max

Mn

P

max

S

max

Als

min

Ti

max

Cu

max

Cr
max
Ni
max
Mo
max
Nb V
AH36 0.18 0.50 0.90-1.60 0.035 0.035 0.015 0.02 0.35 0.20 0.40 0.08 0.02-0.05 0.05-0.10

Note: Generally speaking CE will be ≤ 0.40%. If the delivery condition is TMPC, the CE will be : ≤ 0.38% (thickness ≤ 50mm),≤0.40%( when the thickness >50-100). Ceq% =(C+Mn)/6+(Cr+Mo+V)/5+(Ni+Cu)/15.

AH36 steel plate Mechanical Property


Grade
Rm
(MPa)
Re(MPa) min A% min Akv/J min
AH36 490-630 355 21 E.T °C Thickness (mm)
0 ≤ 50 >50-70 >70-100
L C L C L C
34 24 41 27 50 34

Note: In the list , Rm: .tensile strength,Re: Yield strength,A%: elongation, E.T: experimental temperature,L: lengthways, C: crosswise.

AH36 steel plate Condition Of Delivery


Grade
Fine grains elements category The thickness of steel
≤ 12 >12.5-20 >20-25 >25-35 >35-50 >50-100
AH36 Nb+V or V Plate/
sheet
A(50) N(50),CR(50),TM(50) N(50),CR(25),TM(50)
Profile steel N(50),CR(50),TM(50),AR*(25) -
Al or Al+Ti Plate/
sheet
A(50) AR*(25) -
N(50),CR(50),TM(50) N(50),CR(25),TM(50)
Profile steel A(50) N(50),CR(50),TM(50),AR*(25) -

Note: 1. delivery condition: A =Any ; N=Normalized ; CR=Control Rolled ; TM=TMPC, Temperature - deformation control rolling; AR*= Can be hot rolled with the agreement of Classification Society ; CR*=Can be control rolled with the agreement of Classification Society .
2. The Figure in the ( ) means the sampling volume to do the impact test, the unit is Ton.(-) means without impact test.

AH36 steel plate Contrast in the different standard


ASTM A131M
TOCT 5521 BS LR GB712
AH36 A36 AH36 A36

 

 

AH36 A36 HT Steel Plate SIZE: 10 MM THK X 2000 MM  X 6000 MM ) OF MIN YIELD STRESS 355N/mm2 0AH36 A36 HT Steel Plate SIZE: 10 MM THK X 2000 MM  X 6000 MM ) OF MIN YIELD STRESS 355N/mm2 1

AH36 A36 HT Steel Plate SIZE: 10 MM THK X 2000 MM  X 6000 MM ) OF MIN YIELD STRESS 355N/mm2 2AH36 A36 HT Steel Plate SIZE: 10 MM THK X 2000 MM  X 6000 MM ) OF MIN YIELD STRESS 355N/mm2 3

Hot Tags: ah36 a36 ht steel plate size: 10 mm thk x 2000 mm x 6000 mm ) of min yield stress 355n/mm2, China ah36 a36 ht steel plate size: 10 mm thk x 2000 mm x 6000 mm ) of min yield stress 355n/mm2 suppliers, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS431 Stainless Steel Plate, SS410 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry