AISI/SS 409L Sheet is also known as UNS S40900 or EN 1.4512 which is a stable version of grade 409 that is composed of chromium content and some amount of nitrogen and carbon. This type of stainless steel grade is widely used by manufacturers for manufacturing different applications and equipment. Grade 409L is a low-cost option for the corrosion resistant stainless steel. It even has a good combination of corrosion resistance and heat resistance that is an ideal choice for lightly corrosive applications or the environment.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a240 grade 409l 3.0-40.0mm hot rolled stainless steel plate in China. If you're going to wholesale high quality astm a240 grade 409l 3.0-40.0mm hot rolled stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

AISI/SS 409L Sheet is also known as UNS S40900 or EN 1.4512 which is a stable version of grade 409 that is composed of chromium content and some amount of nitrogen and carbon. This type of stainless steel grade is widely used by manufacturers for manufacturing different applications and equipment. Grade 409L is a low-cost option for the corrosion resistant stainless steel. It even has a good combination of corrosion resistance and heat resistance that is an ideal choice for lightly corrosive applications or the environment.

Chemical Composition of 409L Stainless Steel

Grades

C

Si

Mn

P

S

Cr

Ni

Mo

Ti

Cu

Other

409L

<=0.030

<=0.75

<=0.80

<=0.040

<=0.015

10.50-12.25

-

-

>=6(C+N)

-

-

Mechanical Properties of 409L Stainless Steel

Element

Tensile Strength %

Yield Strength %

Elongation

Hardness (HRB) max

SS 409L

380

170

20

88

Features of AISI/SS 409L Sheet

Corrosion resistance

Excellent resistance to the exhaust gas, high temperature, and atmospheric corrosion

Good formability and excellent flexibility

Low cost

Durability

Grade Specifications for Stainless Steel 409L Sheets

Grade WERKSTOFF NR. UNS JIS
SS 409L 1.4512 S40903 SUH 409L

 

Quick Informations of Our 409L Stainless Steel Plate

Products Name 409L Stainless Steel Plate
Standard ASTM A240/240M-15
Thickness 3.0 - 40.0mm in stock
Size 1500*6000mm or Custom as request
Surface Black or NO.1
Service Cutting

product-317-313product-600-450product-818-614product-800-800

 

FAQ

Q: Can provide OEM/ODM service?

A: Yes. Please feel free to contact us for more details discuss.

Q: How is your Payment Term?

A: Our usual payment methods are T/T, L/C, D/A, D/P, Western Union, Money Gram, payment methods can be negotiated and customized with customers.

Q: Can I get samples before order ?

A: Yes, of course.We can produce by your samples or technical drawings ;

Q: Can I go to your factory to visit?

A: Of course, we welcome customers from all over the world to visit our factory ;

Q:What are the shipping ports?

A:Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.

Hot Tags: astm a240 grade 409l 3.0-40.0mm hot rolled stainless steel plate, China astm a240 grade 409l 3.0-40.0mm hot rolled stainless steel plate suppliers, Corrugated SS Roof Sheet, SS410 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS431 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, 400 2 4360 Alloy Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry