17-4 PH Stainless Steel Sheet
video

17-4 PH Stainless Steel Sheet

17-4 PH steel (AMS 5604) is a grade of martensitic, precipitation-hardening stainless steel with the additions of chromium, nickel, and copper. 17-4 stainless steel has a valuable combination of high strength, good corrosion resistance, and toughness in both base metals and welds. This material provides excellent corrosion resistance (comparable to grade 304) for many medical, chemical, paper, and food processing industries, and it withstands corrosive attacks better than most hardenable stainless steels.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 17-4 ph stainless steel sheet in China. If you're going to wholesale high quality 17-4 ph stainless steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

17-4 PH steel (AMS 5604) is a grade of martensitic, precipitation-hardening stainless steel with the additions of chromium, nickel, and copper. 17-4 stainless steel has a valuable combination of high strength, good corrosion resistance, and toughness in both base metals and welds. This material provides excellent corrosion resistance (comparable to grade 304) for many medical, chemical, paper, and food processing industries, and it withstands corrosive attacks better than most hardenable stainless steels.

 

These properties give designers the ability to add reliability to their products while simplifying fabrication and often reducing their costs. High strength is maintained to approximately 600°F (316°C). 17-4ph has good resistance to stress corrosion cracking at higher aging temperatures.

4 243

Specification Description
Grade 17-4 PH
Standard ASTM A693, AMS 5604, AMS 5622
Thickness 0.4 mm to 100 mm
Width 1000 mm, 1219 mm, 1500 mm, Custom sizes available
Length Custom lengths available, typically up to 6 meters
Surface Finish No. 1, 2B, BA, No. 4, No. 8, HL (Hairline)
Condition Annealed (A), H900, H1025, H1075, H1150, H1150M
Tensile Strength 930 - 1310 MPa (varies with heat treatment condition)
Yield Strength 520 - 1170 MPa (varies with heat treatment condition)
Elongation 8% - 20% (varies with heat treatment condition)
Hardness 28-44 HRC (varies with heat treatment condition)

Also known as Alloy 630, type 17-4PH is the most widely used of all precipitation-hardening steels. Compared to other PH alloys, it requires a simple heat treatment to produce a wide range of properties, including its high strength. It has a slightly higher ferrite content than other PH grades, making it a bit more magnetic. To improve formability, heat treatments may be used before cold working.

Hot Tags: 17-4 ph stainless steel sheet, China 17-4 ph stainless steel sheet suppliers, Corrugated SS Roof Sheet, Stainless Steel 316 316L 316Ti Sheets And Plates, SS410 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry