Alloy 17-4PH Stainless Steel Plate
video

Alloy 17-4PH Stainless Steel Plate

Alloy 17-4PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 572°F /300°C), and corrosion resistance. Mechanical properties can be optimized with heat treatment. Very high yield strength up to 1100-1300 MPa (160-190 ksi) can be achieved.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy 17-4ph stainless steel plate in China. If you're going to wholesale high quality alloy 17-4ph stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 17-4PH Stainless Steel Plate

Product Introduction

Alloy 17-4PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 572°F /300°C), and corrosion resistance. Mechanical properties can be optimized with heat treatment. Very high yield strength up to 1100-1300 MPa (160-190 ksi) can be achieved.

Alloy 17-4PH (UNS S17400), Type 630, is a chromium-nickel-copper precipitation-hardening martensitic stainless steel with an addition of niobium. 17-4PH combines high strength and hardness with good corrosion resistance.

The alloy is furnished in the solution annealed condition (Condition A). It should not be used at temperatures above 572°F (300°C) or for cryogenic service. Optimal mechanical properties can be obtained by subjecting the alloy to age hardening heat treatments. Heat treatment in the 900°F (482°C) range produces the highest strength.

The corrosion resistance of Alloy 17-4PH is comparable to 304 stainless steel in most environments, and is generally superior to the 400 series stainless steels. It is used in applications where the combination of moderate corrosion resistance and unusually high strength are required.

Alloy 17-4PH can be easily welded and processed by standard shop fabrication practices. It is magnetic.

Hot Tags: alloy 17-4ph stainless steel plate, China alloy 17-4ph stainless steel plate suppliers, SS410 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, SS409 Stainless Steel Welded Pipe, 1 4510 Stainless Steel Patterned Plate, Corrugated SS Roof Sheet, SS431 Stainless Steel Plate