Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel plate 321h in China. If you're going to wholesale high quality stainless steel plate 321h made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Available thicknesses for Alloy 321/321H:
| 3/16" | 1/4" | 5/16" | 3/8" | 1/2" | 5/8" | 3/4" | 7/8" | 1" | 1 1/8" |
|---|---|---|---|---|---|---|---|---|---|
| 4.8mm | 6.3mm | 7.9mm | 9.5mm | 12.7mm | 15.9mm | 19mm | 22.2mm | 25.4mm | 28.6mm |
| 1 1/4" | 1 1/2" | 1 3/4" | 2" | 2 1/4" | 2 1/2" | 2 3/4" | 3" | 3 1/2" | 4" |
| 31.8mm | 38.1mm | 44.5mm | 50.8mm | 57.2mm | 63.5mm | 69.9mm | 76.2mm | 88.9mm | 101.6mm |
Alloy 321 stainless steel plate is also advantageous for high temperature service because of its good mechanical properties. Alloy 321 stainless steel plate offers higher creep and stress rupture properties than Alloy 304 and, particularly, Alloy 304L, which might also be considered for exposures where sensitization and intergranular corrosion are concerns.
General Properties
Alloy 321 (UNS S32100) is titanium stabilized austenitic stainless steel plate with good general corrosion resistance. It has excellent resistance to intergranular corrosion after exposure to temperatures in the chromium carbide precipitation range of 800 - 1500°F (427 - 816°C). The alloy resists oxidation to 1500°F (816°C) and has higher creep and stress rupture properties than alloys 304 and 304L. It also possesses good low temperature toughness.
Alloy 321H (UNS S 32109) stainless steel plate is the higher carbon (0.04 - 0.10) version of the alloy. It was developed for enhanced creep resistance and for higher strength at temperatures above 1000oF (537°C). In most instances, the carbon content of the plate enables dual certification.
Alloy 321 stainless steel plate cannot be hardened by heat treatment, only by cold working. It can be easily welded and processed by standard shop fabrication practices.




Fabrication Data
Alloy 321 stainless steel plate can be easily welded and processed by standard shop fabrication practices.
Cold Forming
The alloy is quite ductile and forms easily.
Hot Forming
The high sulfur content of Alloy 303 also has a detrimental impact on hot workability. If hot forming is required, once again, 304 should be considered as an alternate selection.
Machining
The cold work hardening rate of 321 stainless steel plate makes it less machinable than 410 stainless steel, but similar to 304. The table below provides relevant machining data.
| Operation | Tool | Lubrication | CONDITIONS | |||||
|---|---|---|---|---|---|---|---|---|
| Depth-mm | Depth-in | Feed-mm/t | Feed-in/t | Speed-m/min | Speed-ft/min | |||
| Turning | High Speed Steel | Cutting Oil | 6 | .23 | 0.5 | .019 | 12-16 | 39-52 |
| Turning | High Speed Steel | Cutting Oil | 3 | .11 | 0.4 | .016 | 18-23 | 59-75 |
| Turning | High Speed Steel | Cutting Oil | 1 | .04 | 0.2 | .008 | 23-28 | 75-92 |
| Turning | Carbide | Dry or Cutting Oil | 6 | .23 | 0.5 | .019 | 67-76 | 220-249 |
| Turning | Carbide | Dry or Cutting Oil | 3 | .11 | 0.4 | .016 | 81-90 | 226-295 |
| Turning | Carbide | Dry or Cutting Oil | 1 | .04 | 0.2 | .008 | 99-108 | 325-354 |
| Depth of cut-mm | Depth of cut-in | Feed-mm/t | Feed-in/t | Speed-m/min | Speed-ft/min | |||
| Cutting | High Speed Steel | Cutting Oil | 1.5 | .06 | 0.03-0.05 | .0012-.0020 | 16-21 | 52-69 |
| Cutting | High Speed Steel | Cutting Oil | 3 | .11 | 0.04-0.06 | .0016-.0024 | 17-22 | 56-72 |
| Cutting | High Speed Steel | Cutting Oil | 6 | .23 | 0.05-0.07 | .0020-.0027 | 18-23 | 59-75 |
| Drill ø mm | Drill ø in | Feed-mm/t | Feed-in/t | Speed-m/min | Speed-ft/min | |||
| Drilling | High Speed Steel | Cutting Oil | 1.5 | .06 | 0.02-0.03 | .0007-.0012 | 9-13 | 29-42 |
| Drilling | High Speed Steel | Cutting Oil | 3 | .11 | 0.05-0.06 | .0020-.0024 | 11-15 | 36-49 |
| Drilling | High Speed Steel | Cutting Oil | 6 | .23 | 0.08-0.09 | .0031-.0035 | 11-15 | 36-49 |
| Drilling | High Speed Steel | Cutting Oil | 12 | .48 | 0.09-0.10 | .0035-.0039 | 11-15 | 36-49 |
| Feed-mm/t | Feed-in/t | Speed-m/min | Speed-ft/min | |||||
| Milling Profiling | High Speed Steel | Cutting Oil | 0.05-0.10 | .002-.004 | 11-21 | 36-69 | ||
FAQ
Q: Can I get your best price?
A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.
Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to quantity.
Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight.
Q: What is your terms of payment ?
A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable
Hot Tags: stainless steel plate 321h, China stainless steel plate 321h suppliers, hastelloy material piping alloy, , alloy piping, , incoloy seamless pipe
You Might Also Like
Send Inquiry