1.4477 1.4512 Stainless Steel Sheet
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4477 1.4512 stainless steel sheet in China. If you're going to wholesale high quality 1.4477 1.4512 stainless steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Products Description
1.4477 1.4512 Stainless Steel Sheet
Duplex (ferrite-austenite) stainless steels maintain properties both ferritic steel and austenitic steel and possess the feature of superplasticity, which have each half austenitic and ferritic structures. Under the circumstances of lower carbon content, chromium content 18% ~ 28%, Nickel content 3%~10%. Some other steels contain the alloy elements - Mo, Cu, Si, Nb, Ti, N and so on. Those steels possess the properties of austenite and ferrite steels. Compared with ferritic steels, duplex stainless steels have good plasticity and toughness, non-room temperature fragility, intergranular corrosion resistance and weldability, and also maintain the features of ferritic stainless steel 475℃ frangibility, a higher heat conductivity coefficient, superplasticity. Compared with austenitic stainless steel, duplex stainless steel possess high strength, intergranular corrosion resistance and excellent chloride stress corrosion resistant. and also superior pitting resistance.
Products Properties
Chemical composition(mass fraction)(wt.%) of the 1.4477
| C | Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|
| ≤0.030 | 0.50 | 0.80-1.50 | 0.030 | 0.015 | 28.0-30.0 | 5.80-7.50 | 1.50-2.60 | N 0.30-0.40 Cu ≤ 0.80 |
Mechanical properties / Mechanische Eigenschaften / Caracteristiques mecaniques of grade 1.4477
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 165 (≥) | 198 (≥) | 21 | 34 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 144 |
1.4477 1.4512 Stainless Steel Sheet

EN 1.4477 stainless steel is a duplex stainless steel formulated for primary forming into wrought products. 1.4477 is the EN numeric designation for this material. X2CrNiMoN29-7-2 is the EN chemical designation.
It can have a fairly high tensile strength among wrought duplex stainless steels. In addition, it has a fairly low thermal conductivity and can have a moderately low ductility.
FAQ
Q:Can you assist me in importing steel products for the first time?
A:Yes, we have shipping agent who will arrange the shipment with you.
Q: What is your delivery time?
A:Within 7 working days after receiving your balance payment.
Q:About stainless seamless pipe product prices?
A:Prices vary from period to period due to cyclical changes in the price of raw materials.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: What is your terms of payment ?
A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable
Hot Tags: 1.4477 1.4512 stainless steel sheet, China 1.4477 1.4512 stainless steel sheet suppliers, SS410 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, Corrugated SS Roof Sheet
You Might Also Like
Send Inquiry