Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 301 stainless steel sheet in China. If you're going to wholesale high quality 301 stainless steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Type 301 Stainless Steel is an austenitic chromium-nickel stainless steel that provides high strength and good ductility when cold worked. The chromium and nickel contents are lowered to increase the cold work-hardening rate. This generates higher tensile strengths when cold rolled with a lower loss of ductility than with Types 302 and 304. The grade is essentially non-magnetic when annealed. When cold worked, it becomes slightly more magnetic than other standard austenitic stainless steels.

| Element | Type |
|---|---|
| Carbon | 0.15 max. |
| Manganese | 2.00 max. |
| Sulfur | 0.030 max. |
| Phosphorus | 0.045 max. |
| Silicon | 0.75 max. |
| Chromium | 16.00 – 18.00 |
| Nickel | 6.00 – 8.00 |
| Nitrogen | 0.10 max. |
Hot Tags: 301 stainless steel sheet, China 301 stainless steel sheet suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, Corrugated SS Roof Sheet, SS410 Stainless Steel Plate, SS431 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate