1.4016 Stainless Steel Sheet #4 Finish
video

1.4016 Stainless Steel Sheet #4 Finish

Stainless steel type 1.4016 is also commonly known as grade 430. Type 430 ss sheet combines good corrosion resistance with good formability and ductility.It is a ferritic, non-hardenable plain Chromium stainless steel with excellent finish quality.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4016 stainless steel sheet #4 finish in China. If you're going to wholesale high quality 1.4016 stainless steel sheet #4 finish made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

1.4016 stainless steel sheet #4 finish is the brushed finish commonly seen on kitchen appliances and backsplashes. Stainless 1.4016 Plate #4 finish has a PVC film on one side to help protect against scratching during fabrication and installation. Our 1.4016 SS sheet metal meets the criteria for both the #3 and #4 finish.

 

Chemical Composition of SS 430 sheet :

C

Si

Mn

P≤

S≤

Cr

Mo

Ni

Other

430

≤0.08

≤1.00

≤2.00

0.045

16_18

0

-

8-


Grade 430 also has excellent resistance to nitric attack, which makes it well suited to use in chemical applications. The most popular applications for 430 are in domestic appliances and decorative trim.
Property data given in this document is typical for flat rolled products covered by EN 10088-2:2005. ASTM, EN or other standards may cover products sold. It is reasonable to expect specifications in these standards to be similar but not necessarily identical to those given in this datasheet.

 

SS PALTE

Applications of 1.4016 Stainless Steel Sheet

  • Low cost sinks
  • Decorative trim
  • White & brown Goods (washing machines, dishwashers, cookers)
  • Refrigerators
  • Stove element supports
  • Scientific apparatus
  • Fasteners
  • Flue linings
  • Automotive trim
  • Hinges

 

Stainless Sheet - Up To 8mm Thick

Mechanical Property Value
Proof Stress 260 Min MPa
Tensile Strength 450 - 600 MPa
Elongation A50 mm 20 Min %


SS Plate - Over 8mm to 13.5mm / Thick

Mechanical Property Value
Proof Stress 240 Min MPa
Tensile Strength 450 - 600 MPa
Elongation A50 mm 18 Min %


Stainless Steel Plate - Over 13.5mm to 25mm Thick

Mechanical Property Value
Proof Stress 240 Min MPa
Tensile Strength 430 - 630 MPa
Elongation A50 mm 20 Min %

 

CUSTOMER VISIT

GNEE Steel Group Is Your Wise Choice

GNEE

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

 

Hot Tags: 1.4016 stainless steel sheet #4 finish, China 1.4016 stainless steel sheet #4 finish suppliers, SS410 Stainless Steel Plate, Corrugated SS Roof Sheet, ASTM A240 Grade 431 10mm Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate