High resistance to corrosion in industrial and domestic environments. Good strength. Reasonable resistance to impact when tempered and hardened. Shows resistance to many chemicals.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4028 1.4541 plates of middle thickness in China. If you're going to wholesale high quality 1.4028 1.4541 plates of middle thickness made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Products Description

1.4028 1.4541 Plates Of Middle Thickness

Applications:

  • Because of its properties, stainless steel type 420J2 has a wide range of applications including:
  • Surgical instruments
  • Daggers and swords
  • Budget knives and diving knives
  • Haircutting scissors and domestic scissors

 

Products Properties

 

Chemical composition

Chemical composition % of steel X30Cr13 (1.4028): EN 10088-2-2005

C Si Mn P S Cr
0.26 – 0.35 max 1 max 1.5 max 0.04 max 0.015 12-14

1.4028 1.4541 Plates Of Middle Thickness

 Medium and Thick Plate

Type 420J2 stainless steel is martensitic steel, which is inexpensive and very resistant to corrosion. It offers corrosion resistance both in industrial and domestic environments, as well as in the mild atmosphere.It provides resistance to many chemicals, acids, petroleum products, steam, and household cleaners. Type 420J2 is the preferred stainless-steel choice for knife manufacturers.In comparison with 440 grades, stainless-steel type 420J2 provides better strength and good resistance to impact when it is in tempered and hardened conditions.

Grade 321 stainless steel (1.4541) is a heat resistant grade supplied into numerous industry sectors. The key property of this grade is the added titanium content (5 x C%) stabilising the material and making its resistance to carbide precipitation when exposed to high temperatures and resistance to oxidation its main characteristics.

Customer Case

medium-thick steel plate

FAQ

 

Q:About stainless pipe product prices?
A:Prices vary from period to period due to cyclical changes in the price of raw materials.

Q:What shipping ports are there?

A:We normally ship from Shanghai,Tianjin, Qingdao, and Ningbo ports

Q:What are your payment terms?

A:30% T/T in advance and 70% balance before shipment or based on BL copy or LC at sight.

Q:What about product pricing information?

A:Prices vary due to changes in raw material prices on a regular basis.

Q:Is it possible to send samples?

A:Of course, we offer free samples and express shipping to customers all over the world.
Q:Do you offer a service for customized products?

A:Yes, we can produce according to your specifications and drawings.

Hot Tags: 1.4028 1.4541 plates of middle thickness, China 1.4028 1.4541 plates of middle thickness suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, 1 4510 Stainless Steel Patterned Plate, SS409 Stainless Steel Welded Pipe, SS410 Stainless Steel Plate, SS431 Stainless Steel Plate, Corrugated SS Roof Sheet

Send Inquiry

whatsapp

Phone

E-mail

Inquiry