1.4016 1.4550 Wire Draw Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4016 1.4550 wire draw plate in China. If you're going to wholesale high quality 1.4016 1.4550 wire draw plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Products Description
1.4016 1.4550 Wire Draw Plate
Key Features:
- Plain chromium stainless steel with good corrosion resistance
- Due to nitric acid resistance, it is used in several chemical applications
- Resistance to corrosion is maximized in buffed or well-polished condition
- Becomes brittle at room temperature if heated for a long time at temperatures between 752-1112 o This issue is solved by annealing
- Good machining properties, but galling can happen
- Difficult to execute rigorous operations, due to low ductility
Products Properties
Chemical Composition
| Chemical Element | % Present |
|---|---|
| Carbon (C) | 0.0 - 0.08 |
| Chromium (Cr) | 16.00 - 18.00 |
| Manganese (Mn) | 0.0 - 1.00 |
| Silicon (Si) | 0.0 - 1.00 |
| Phosphorous (P) | 0.0 - 0.04 |
| Sulphur (S) | 0.0 - 0.02 |
| Iron (Fe) | Balance |
1.4016 1.4550 Wire Draw Plate

Type 430 stainless steel(1.4016) is ferritic steel, with low carbon content and plain chromium. Type 430 provides good resistance to corrosion in environments that are mildly corrosive and good oxidation in conditions of elevated temperatures. Due to its resistance to nitric acid, it can be extremely useful in certain chemical applications.Type 430 offers good formability and weldability, but it is not recommended for hard service. It shows good machining properties, although galling can happen.
347 material(1.4550 stainless steel )is a high temperature grade and it is designed for temperatures between 400 to 800 degree. 347 stainless can not be heat threated and it has a similar corrosion resistance to 321 and 304 grade stainless steels. 347 stainless is similar to 321 (1.4541) grade for many applications and this grade can weld easiliy. The most important elements in 1.4550 material are niobium and tantalum, which makes this grade have more stabilized structure. 347 stainless steel used in chemical industry, food production facilities, food storage equipment, oil refinery parts, waste treatment plants.
Customer Case

FAQ
Q:Can I pay you a visit at your factory?
A:Customers from all around the world are welcome to visit our factory.
Q:Can you assist me in importing steel products for the first time?
A:Yes, we have shipping agent who will arrange the shipment with you.
Q: What is your delivery time?
A:Within 7 working days after receiving your balance payment.
Q:What shipping ports are there?
A:We normally ship from Shanghai,Tianjin, Qingdao, and Ningbo ports
Q:What are your payment terms?
A:30% T/T in advance and 70% balance before shipment or based on BL copy or LC at sight.
Hot Tags: 1.4016 1.4550 wire draw plate, China 1.4016 1.4550 wire draw plate suppliers, 1 4510 Stainless Steel Patterned Plate, SS409 Stainless Steel Welded Pipe, SS410 Stainless Steel Plate, Corrugated SS Roof Sheet, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS431 Stainless Steel Plate