0.5*1220x2440mm Stainless Steel Water Ripple Sheet Plate 201 (Medium Ripple) ROSE GOLD
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 0.5*1220x2440mm stainless steel water ripple sheet plate 201 (medium ripple) rose gold in China. If you're going to wholesale high quality 0.5*1220x2440mm stainless steel water ripple sheet plate 201 (medium ripple) rose gold made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
0.5*1220x2440mm Stainless Steel Water Ripple Sheet Plate 201 (Medium Ripple) ROSE GOLD
Description
| Technique: | Cold Rolled,hot Rolled,rerolling | Technology: | Cold Rolled.hot Rolled |
|---|---|---|---|
| Normal Size: | 1220*2440 | Hole Diameter: | 0.05-10mm |
| Finish: | 2B | Port: | Shanghai |
| Grade: | 304/316L | Mill: | TISCO |
| Thickness Tolerance: | Within 5% | Key Word: | 304 Stainless Steel Strapping Band |
| Tech: | Cold Rolled | Wdith: | 10-2000mm |
| Trade Terms: | FOB CIF CFR EXW | Cold Rolled Thickness: | 0.3-4mm |
0.5*1220x2440mm Stainless Steel Water Ripple Sheet Plate 201 (Medium Ripple) ROSE GOLD
Water Ripple Sheet Hot Rolled Cold Rolled Decorative Stainless Steel Sheet
Stainless Steel Water Ripple Decorative Sheet
Stainless steel water ripple sheets are widely used in wall and ceiling decoration due to its strong decorative and fashion effect. It has the advantages of easy to clean, maintenance free and fingerprint-free, etc. If there are stains, just wipe them with a cloth.
Application
As a fashionable artistic interior decoration sheet, metal corrugated sheet is made of metal stainless steel sheet through machine stamping and cold drawing. It is currently widely used in indoor and outdoor decoration including high-end residences and various commercial spaces. When a large area of bright silver water ripple ceiling is used, the entire space can be made transparent, especially when the light reflects the changes in depth, it deepens the sense of spatial hierarchy.
Classification
The surface of the ordinary metal corrugated sheet is flat, and the refracted image is also uniform and uniform. But if the metal plate is beaten with a hammer, the surface will become uneven, and the refracted picture can present a visual three-dimensional effect. Through different percussion methods, the metal water ripple sheet can be divided into three categories: large water ripples, small water ripples, and water scale patterns. Water ripple surface treatment methods include bright, brushed, gold, rose gold, black titanium, champagne gold, and sapphire blue.
| Type | Water Ripple Stainless Steel Sheet |
| Thickness | 0.3mm - 3.0mm |
| Standard Sizes | 1000*2000mm, 1219*2438mm, 1500*3000mm |
| Grade | 304, 316L, 430, 201 etc. |
| Finish | Stamped Finish |
| Other Finished | NO.4, Hairline, Mirror, PVD Color, Etched, Embossed, Polished Pattern, Sandblasted, Vibration, Lamination etc. |
| Mill Origin | POSCO, BAOSTEEL, YONGJIN, JISCO, TISCO etc. |
| Service | Customized Sizes and Colors, Free Samples |
| Fabrication | Shearing, Bending, Grooving |
| Chemical Composition | ||||
| Grade | SUS304 | SUS316L | SUS430 | SUS201 |
| Elong(%) | ≥40 | 30 | >22 | 50-60 |
| Hardness | ≤200HV | ≤200HV | <200HV | 100HRB, 230HV |
| Cr(%) | 18-20 | 16-18 | 16-18 | 16-18 |
| Ni(%) | 8-10 | 10-14 | ≤0.6 | 0.5-1.5 |
| C% | ≤0.08 | ≤0.07 | ≤0.12 | ≤0.15 |



FAQ
Q1: How many countries you already exported ?
A1: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan, etc.
Q2: How can I get some samples?
A2: Small samples in store and can provide the samples for free. Catalgue is available, most patterns we have ready samples in stock. Customized samples will be taken about 5-7days.
Q3: What is the MOQ?
A3: Stainless steel coils 3 tons. Pattern sheets 10pcs.
Q4: What is the delivery?
A4: Sample order's delivery time is 5-7 days. Container orders are about 15-20 days.
Q5: How does your company do regarding quality control?
A5: BV and SGS certificates, production process followed the ISO9000 system.
Q6: How to protect the sheets?
A6: Two white and black PE layers to cover the surface, each layer is 70 micro (Total 140 micro), laser PVC is also workable.( Novacel or Poli-film brand )
Q7: What is the application about your products?
A7: 1. Elevator door and cabin or escalator's side-wall. 2. Wall cladding inside or outside meeting room and restaurant. 3. Facade when cladding over something, like columns in the lobby. 4. Ceiling in the supermarket. 5. Decorative draws in some entertainment places.
Q8: How long can you guarantee for this product and finish?
A8: Color guarantee for more than 10 years. Original materials quality certificate can be provided.
Tag:
stainless steel panels,
stainless steel metal sheet,
stainless steel plate
Hot Tags: 0.5*1220x2440mm stainless steel water ripple sheet plate 201 (medium ripple) rose gold, China 0.5*1220x2440mm stainless steel water ripple sheet plate 201 (medium ripple) rose gold suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, SS409 Stainless Steel Welded Pipe, Corrugated SS Roof Sheet, SS410 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate
You Might Also Like
Send Inquiry