Plate Grade Hastelloy C-276 Alloy ASTM B575 UNS N10276 Alloy Plate
video

Plate Grade Hastelloy C-276 Alloy ASTM B575 UNS N10276 Alloy Plate

Specification details Type Cold Rolled Nickel alloys strips/ coils Grade HC-276, HC-22, ALLOY 600, ALLOY 625, ALLOY 718, ALLOY X750 <> HASTELLOY, HAYNES, INCONEL, INCOLOY, MONEL, RENE 41, WASPALOY Finish Roll-Up(Hard),Skin pass(2B) others. Surface finish Bright, Dull, Hair Line(HL), others. Thickness 0.030 - 1.00mm Width 3.0 - 300mm Length Coil (strip) or sheet (Length100~2,000mm) ID φ300,400,500mm (Inner Core) MOQ 50kg ≤
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of plate grade hastelloy c-276 alloy astm b575 uns n10276 alloy plate in China. If you're going to wholesale high quality plate grade hastelloy c-276 alloy astm b575 uns n10276 alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Plate Grade Hastelloy C-276 Alloy ASTM B575 UNS N10276 Alloy Plate

Description

Material: Stainless Steel Shape: Flat Plate Sheet
Thickness: 1-30mm Width: 10mm-1500mm
Length: 200-12000mm Surface: 2B NO.1

Hastelloy C276 Plate

While the Alloy C276 Sheet has a higher rate of work hardening in comparison to its austenitic counterpart grades, an in processing annealing may be required if the Nickel Alloy C276 Sheet is to be work hardened to a higher degree. A solution annealing process may be required if the Nickel C276 Strip undergoes a deformation rate of more than 15%.

ASTM B575 Alloy C276 Plate is resistant to general corrosion, stresscorrosion cracking, pitting and crevice corrosion in a broad range of severe environments. Alloy C276 Hastelloy plate has exceptional resistance to sulfuric acid and hydrochloric acid.

Specification and Material grade of C276 Hastelloy plate

ASTM Specification ASTM B127 / ASME SB127
Standard MSRR, AMS, BS
Length & Sizes 1000 mm x 2000 mm, 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1250mm x 2500mm, 1500mm x 3000mm to 6000mm, 2000mm x 4000mm to 6000mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm, 2m, 2.44m, 3m, 36" X 120" or 48" X 144", 4' x 8', Cut to size available
Thickness 0.1mm to 100 mm Thk
Width 10-2500mm
Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.
Temper Annealed
Condition Polished on both sides
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Stock in form of Plate, Sheet, Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Clad Plate, Rolling Sheet, Flat Sheet, Rolling Plate, Flat Shim, Blank (Circle), hot rolled, cold rolled, annealed, soft annealed, descaled, sheared, tread plate, Checker Plate
Value Added Service Cladding, Heat Treatment, Annealed, Pickling, Polish, Rolling, Cutting, Bending, Forging, Minor Fabrication Etc.
Dealers & Distributor of SAIL, ESSAR, JINDAL, TATA, BHUSHAN, INDIAN, POSCO, JISCO, TISCO, LISCO, BAOSTEEL IMPORTED material
Test Report

Raw Materials Certificate

EN 10204/3.1B

100% Radiography Test Report

High special strength, high melt point

Third Party Inspection Report, etc

Excellent corrosive resistance, good thermal resistance

Customer support after-sales service

Strict Control from Raw Material to Finished

Profiling

To provide a full profiling service we use numerous profiling methods including:

Plasma Plate Cutting

Laser Plate Cutting

Oxy-propane Flame Cutting

Specialized in

material under 3/16 " [5.00 mm] in thickness and 24" [600 mm] and over in width

material 3/16" [5.00 mm] and over in thickness and over 10" [250 mm] in width

cold-rolled material under 3/16" [5.00 mm] in thickness and under 24" [600 mm] in width

Free Quote, Inquiry answered within 24 hours

We offer a comprehensive services designed to add value to your project: plasma cutting, waterjet cutting, laser cutting, bending and mechanical processing, edge preparation, welding, sawing and shearing.

Price List of C276 Hastelloy Sheet

Price of Hastelloy C276 Plate C276 Alloy Plate Price in India (INR) Nickel Alloy C276 Plate Price in USD ASTM B575 UNS N10276 Plate Price in UAE Dirham
NICKEL ALLOY PLATES CONF. TO SPECN.SB-575 UNS-N10276 HASTELLOY C-276 SIZE(MM): 16 X 2000 X 7500 INR 1,380 $18.55 68.12 UAE Dirham
NICKEL ALLOY PLATE HASTELLOY C 276 0.6*385*940 mm INR 3,047 $40.95 150.42 UAE Dirham
HASTELLOY(R)C - 276 ALLOY PLATE 0.1875 IN THK, 48.0000 IN WIDE, 59.0600 IN LONG NICKEL ALLOY INR 1,815 $24.39 89.60 UAE Dirham
HASTELLOY (R) C-276 ALLOY PLATE 0.5 THK, 39.3700 WIDE,48.0300 INR 2,130 $28.63 105.15 UAE Dirham

Available Types of UNS N10276 Hastelloy C276 Plate

Alloy Hastelloy C276 Shim Stock
Alloy Hastelloy C276 Shim Stock

DIN 17750 Perforated Sheet
DIN 17750 Perforated Sheet

Alloy Hastelloy C276 Shim Stock
VdTüV 400/12.98 Chequered Plate

ASME SB575 UNS N10276 Coil
ASME SB575 UNS N10276 Coil

2.4819 Hastelloy C276 Hot Rolled Plate
2.4819 Hastelloy C276 Hot Rolled Plate

ASME SB575 UNS N10276 Coil
ASME SB575 UNS N10276 Coil

Hastelloy C276 Din 2.4819 Cold Rolled Sheet
Hastelloy C276 Din 2.4819 Cold Rolled Sheet

ISO 6208 Shim Sheet
ISO 6208 Shim Sheet

ASTM B575 Alloy C276 Strip
ASTM B575 Alloy C276 Strip

Hastelloy C276 Superalloy Mesh Plate
Hastelloy C276 Superalloy Mesh Plate

VdTüV 400/12.98 Chequered Plate
VdTüV 400/12.98 Chequered Plate

C276 Hastelloy plate
C276 Hastelloy plate

15.9mm Alloy C276 Plate
15.9mm Alloy C276 Plate

Hastelloy Alloy C276 Checker Plate
Hastelloy Alloy C276 Checker Plate

ISO 6208 Shim Sheet
ISO 6208 Shim Sheet

C276 Hastelloy Shim Sheet
C276 Hastelloy Shim Sheet

DIN 17750 Perforated Sheet
DIN 17750 Perforated Sheet

ASTM B575 Alloy C276 Sheet
ASTM B575 Alloy C276 Sheet

Hastelloy C276 Nickel Alloy Cold Rolled Plate
Hastelloy C276 Nickel Alloy Cold Rolled Plate

Hastelloy Alloy C276 0.5mm thick x 250mmx250mm Plate
Hastelloy Alloy C276 0.5mm thick x 250mmx250mm Plate

ASTM B575 Hastelloy C276 Sheet
ASTM B575 Hastelloy C276 Sheet

5.0x2400x6000 mm ASTM B575 N10276 annealed Plate
5.0x2400x6000 mm ASTM B575 N10276 annealed Plate

ASME sB906 C276 Hastelloy Strip
ASME sB906 C276 Hastelloy Strip

UNS N10276 Hastelloy C276 Foil
UNS N10276 Hastelloy C276 Foil

Alloy Hastelloy C276 Coil
Alloy Hastelloy C276 Coil

ASTM B906 Alloy C276 Foil
ASTM B906 Alloy C276 Foil

UNS N10276 Plate
UNS N10276 Plate

Alloy C276 Nickel Clad Plate
Alloy C276 Nickel Clad Plate

ASTM B906 Alloy C276 Foil
ASTM B906 Alloy C276 Foil

UNS N10276 Hastelloy C276 Chequered Plate
UNS N10276 Hastelloy C276 Chequered Plate

Alloy Hastelloy C276 Strip Tape
Alloy Hastelloy C276 Strip Tape

ASTM B575 Alloy C276 Perforated Sheet
ASTM B575 Alloy C276 Perforated Sheet

ASTM B575 Hastelloy C276 Sheet
ASTM B575 Hastelloy C276 Sheet

C276 Hastelloy 0.5mm thick x 1000mmx2000mm Plate
C276 Hastelloy 0.5mm thick x 1000mmx2000mm Plate

UNS N10276 Plate
UNS N10276 Plate

ASME sB906 C276 Hastelloy Strip
ASME sB906 C276 Hastelloy Strip

2.4819 Hastelloy C276 Sheet
2.4819 Hastelloy C276 Sheet

SB 575 Hastelloy C276 Strip
SB 575 Hastelloy C276 Strip

Hastelloy C276 SB575 4mm Thick Plate
Hastelloy C276 SB575 4mm Thick Plate

Hastelloy Alloy C276 Sheet
Hastelloy Alloy C276 Sheet

2.4819 Alloy C276 Flat Plate
2.4819 Alloy C276 Flat Plate

Haynes Alloy C276 N10276 Polished Plate
Haynes Alloy C276 N10276 Polished Plate

ASTM B575 Alloy C276 Plate
ASTM B575 Alloy C276 Plate

Alloy C276 Hastelloy plate
Alloy C276 Hastelloy plate

ASME SB575 Hastelloy C276 Plate Manufacturers, Hot Rolled JIS NW 6022 Plate exporter in India, 2B/ BA/ HL/ NO.1 finish ASTM B575 Hastelloy C276 Shim Sheets supplier, Check Hastelloy UNS N10276 Polished Plates Sizes

Specification and grade of Hastelloy Alloy C22 Plate/ Sheet

UNS: N10276
Specifications: ASTM B575, ASTM B906
international Specifications: ISO 6208, DIN 17750, VdTüV 400/12.98

Ready Stock of C276 Hastelloy Plate

Hastelloy C276 Chequered Plate C276 Hastelloy Quarto Plate
Nickel Alloy C276 Clad Plate ASTM B575 UNS N10276 Tisco Plate
Hastelloy DIN 2.4819 Chequer Plate Hastelloy Alloy C276 Tread Plate
ASTM B575 UNS N10276 Checker Plate Nickel C276 Polished Plate
Hastelloy Alloy C276 Plate Mirror Finish Nickel Alloy C276 Chequered Plate
Nickel C276 Plate Brushed Finish Hastelloy C276 Hot Rolled Sheet
Nickel Alloy C276 10mm Plate ASTM B575 UNS N10276 Cold Rolled Sheet
Hastelloy C276 1/4 Inch Plate Hastelloy UNS N10276 Perforated Sheet
Hastelloy UNS N10276 Plate Alloy C276 Rolling Plate
C276 Hastelloy Hot Rolled Plate Nickel C276 Perforated Plate
Alloy C276 Cold Rolled Plate Hastelloy 2.4819 Bbq Plate
Nickel C276 Plate 2b Finish Nickel Alloy C276 Diamond Plate
Alloy Hastelloy C276 Plate Hastelloy C-276 UNS N10276 Cold Rolled Plate
ASTM B575 C276 Hastelloy 2D Plate Hastelloy UNS N10276 Polished Cold Drawn Plate
Hastelloy C276 Alloy Strip Tape Hastelloy C276 N10276 Slitting Coil
Alloy C276 Hastelloy Hot Rolled Plate Hastelloy UNS N10276 Polished Cold Drawn Plate
C276 Hastelloy Shim Sheet 2.4819 Alloy C276 Flat Plate
Hastelloy C276 Alloy Strip Tape Hastelloy C276 ASTM B575 Polish Plate
Alloy C276 Hastelloy Hot Rolled Plate Hastelloy C276 Circle
Hastelloy 2.4819 Plate Mill Finish Hastelloy DIN 2.4819 Thin Plate
ASTM B575 UNS N10276 Custom Cut Plate Alloy C276 Sheet
Hastelloy UNS N10276 Checkered Plate Hastelloy C276 Laser Cut Plate
Alloy C276 Embossed Plate Hastelloy UNS N10276 Plasma Cutting Plate
C276 Alloy Plate Stockholder. Laser cutting Hastelloy UNS N10276 Coils wholesaler, Hastelloy C276 Cold Rolled Plates suppliers in India, 0.6mm thick 2B finish Hastelloy Werkstoff No 2.4819 Sheets, Hastelloy UNS N10276 Hot Rolled Plates stockholder.

Alloy C276 Plate Physical Properties

Properties Metric Imperial
Density 8.89 g/cm³ 0.321 lb/in³
Melting point 1371°C 2500°F

Leading Stockholder of Alloy C276 Plate/ Sheet

C276 Hastelloy Hot Rolled Plate

C276 Hastelloy Hot Rolled Plate

 

Hastelloy UNS N10276 Perforated Sheet

Hastelloy UNS N10276 Perforated Sheet

ASTM B575 UNS N10276 Cold Drawn Sheet

ASTM B575 UNS N10276 Cold Drawn Sheet

Nickel Alloy C276 Clad Plate

Nickel Alloy C276 Clad Plate

Hastelloy Alloy C276 Plate Mechanical Strength Table

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Hastelloy C276 8.89 g/cm3 1370 °C (2500 °F) Psi – 1,15,000 , MPa – 790 Psi – 52,000 , MPa – 355 40 %

UNS N10276 Sheet Chemical Composition Standard

Grade C Mn Si S Co Ni Cr Fe Mo P
C276 0.010 max 1.00 max 0.08 max 0.03 max 2.50 max 50.99 min* 14.50 – 16.50 4.00 – 7.00 15.00 – 17.00 0.04 max

Equivalent grades of Nickel C276 Plate/ Sheet

STANDARD WERKSTOFF NR. UNS JIS GOST EN OR
Hastelloy C276 2.4819 N10276 NW 0276 ХН65МВУ NiMo16Cr15W ??760
Distributor of Hastelloy C276 Sheets, Trader of Hastelloy C276 Perforated Coils, Check Alloy C276 Shim Sheet Price Per Kg, Ready Stock of DIN 2.4819 Strips. Hot Rolled C276 Hastelloy Hot Rolled Plates, ASTM B575 Hastelloy C276 Strips manufacturers.

Thermal Properties of ASTM B575 Alloy C276 Plate

Properties Metric Imperial
Thermal expansion co-efficient (@24-93°C/75.2-199°F) 11.2 µm/m°C 6.22 µin/in°F
Thermal conductivity (-168 °C) 7.20 W/mK 50.0 BTU in/hr.ft².°F

Dimension of C276 Hastelloy plate

Hastelloy C276 Plate Imperial Dimensions

Plate Surface finish Gauge (in) Width (max in)
2B – Cold rolled, heat treated, pickled, skin passed Plate 10–24 72*
2D – Cold rolled, heat treated, pickled plate 12–24 60
BA Mexinox only 18–28 48
Polished plate (not brushed) 11–24 60
Temper rolled plate Mexinox only 13–29 48

ASTM B127 Alloy C276 Plate Metric Dimensions

Plate Surface finish Thickness (mm) Width (max mm)
2B – Cold rolled, heat treated, pickled, skin passed plate 0.25–8.0 2032
2D – Cold rolled, heat treated, pickled plate 0.4–6.35 1524
2E – Cold rolled, heat treated, mechanically descaled plate 0.4–8.0 2032
2R – Cold rolled, bright annealed plate 0.25–3.5 1524
2H – Work hardened plate 0.4–6.35 1524
Polished, brushed plate 0.5–4.0 1524

Weight per Unit of JIS NW C276 Plate

Thickness Alloy Plate Weight per Unit Area Density
3/16 inches Hastelloy C276 0.06000 lbs/in²42.184176 kg/m² 0.315 lbs/in³8.72 g/cm³
1/4 inches Hastelloy C276 0.08 lbs/in²56.245568 kg/m² 0.315 lbs/in³8.72 g/cm³
3/8 inches Hastelloy C276 0.121 lbs/in²85.0714216 kg/m² 0.315 lbs/in³8.72 g/cm³
1/2 inches Hastelloy C276 0.161 lbs/in²113.1942056 kg/m² 0.315 lbs/in³8.72 g/cm³
5/8 inches Hastelloy C276 0.196 lbs/in²137.8016416 kg/m² 0.315 lbs/in³8.72 g/cm³
3/4 inches Hastelloy C276 0.235 lbs/in²165.221356 kg/m² 0.315 lbs/in³8.72 g/cm³
7/8 inches Hastelloy C276 0.274 lbs/in²192.6410704 kg/m² 0.315 lbs/in³8.72 g/cm³
1 inches Hastelloy C276 0.313 lbs/in²220.0607848 kg/m² 0.315 lbs/in³8.72 g/cm³
1 1/4 inches Hastelloy C276 0.391 lbs/in²274.9002136 kg/m² 0.315 lbs/in³8.72 g/cm³
1 1/2 inches Hastelloy C276 0.47 lbs/in²330.442712 kg/m² 0.315 lbs/in³8.72 g/cm³
1 3/4 inches Hastelloy C276 0.549 lbs/in²385.9852104 kg/m² 0.315 lbs/in³8.72 g/cm³
2 inches Hastelloy C276 0.627 lbs/in²440.8246392 kg/m² 0.315 lbs/in³8.72 g/cm³
2 1/4 inches Hastelloy C276 0.705 lbs/in²495.664068 kg/m² 0.315 lbs/in³8.72 g/cm³
2 1/2 inches Hastelloy C276 0.784 lbs/in²551.2065664 kg/m² 0.315 lbs/in³8.72 g/cm³
2 3/4 inches Hastelloy C276 0.862 lbs/in²606.0459952 kg/m² 0.315 lbs/in³8.72 g/cm³
3 inches Hastelloy C276 0.941 lbs/in²661.5884936 kg/m² 0.315 lbs/in³8.72 g/cm³

Nickel Alloy C276 Clad Plate Sizes

Size (in inches)

Size (in mm)

.125"

3.18mm

.134"

3.40mm

.156"

3.96mm

.187"

4.75mm

.250"

6.35mm

.312"

7.92mm

.375"

9.53mm

.500"

12.7mm

.625"

15.9mm

.750"

19.1mm

.875"

22.2mm

1"

25.4mm

1.125"

28.6mm

1.250"

31.8mm

1.500"

38.1mm

1.750"

44.5mm

2"

50.8mm

2.500"

63.5mm

3"

76.2mm

2.4819 Hastelloy Plate Stock List

Plate Grade Hastelloy C-276 Alloy ASTM B575 UNS N10276 Alloy Plate 48

 

Hot Tags: plate grade hastelloy c-276 alloy astm b575 uns n10276 alloy plate, China plate grade hastelloy c-276 alloy astm b575 uns n10276 alloy plate suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, SS431 Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS410 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate