ASTM A240 TP405 Plate
video

ASTM A240 TP405 Plate

We create a win-win ASTM A240 TP405 Stainless steel Plate situation for our customers with a sincere attitude and quality service. We are largest exporter and Supplier of ASTM A240 TP405 Stainless steel Plate. We will satisfy you with professional ASTM A240 TP405 Stainless steel Plate service!
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a240 tp405 plate in China. If you're going to wholesale high quality astm a240 tp405 plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

 

GNEE Steel is a known manufacturer,exporter and supplier of ASTM A240 TP405 Plate.We maintain over 800 ton SS 405 Plates in various shape,sizes & coating which makes us one of the largest stockholder 405 SS Plate in China.We are largest exporter and Supplier of ASTM A240 TP405 Stainless steel Plate in China.We offer 405 stainless steel plate in various sizes at best price.We are ISO 9001:2008 certified manufacturer of ASTM A240 Grade 405 plate & now we became Distributor of UNS S40500 Sheet & DIN 1.4002 Stainless Steel Plate. We are well known trader of Stainless Steel 405 Plates in China.We producing stainless steel 405 plate & SS 405 Sheet.

Stainless Steel Sheet Metalss sheet

ASTM A240 SS 405 Plate Specifications

Description ASTM A240 / ASME SA240 Stainless Steel Plates, ASTM A240 Stainless Hot Rolled Plates
Standard ASTM, ASME, BS, DIN, EN
Material 310S, 310, 309, 309S, 316, 316L, 316Ti, 317, 317L, 321, 321H, 347, 347H, 304, 304L,
302, 301, 201, 202, 403, 405, 409, 409L, 410, 410S, 420, 430, 631, 904L, Duplex, etc
Specification Cold rolled: 1219mm * 2438mm (4′ x 8′), 1219mm * 3048mm (4′ x 10′), 1220mm * 2440mm, 1250mm * 2500mm or as your requirement.

Hot rolled: 1500mm * 2000mm, 1000mm * 3000mm, 1500mm * 4000mm, 1500m * 6000mm or as your requiremnt.

Technique Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Form Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Etc.
Surface 2B, 2D, BA, NO. 1, NO. 4, NO.8, 8K, Mirror, Checkered, Embossed, Hair Line, Sand Blast, Brush, Etching
Thickness 0.25-200mm, 0.3mm to 120mm
Width 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm
Length 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, 12000mm
Package Standard Export Seaworthy Package, or as required.
Value Added Services Cladding,Heat Treatment,Annealed, Pickling, Polish,Rolling,Cutting,Bending,Forging,Minor Fabrication Etc.
MTC Mill Test Certificate, Available as per EN 10204 3.1


ASTM A240 Stainless Steel 405 Sheet Chemical Composition

Element Content (%)
Iron, Fe 85
Chromium, Cr 13
Manganese, Mn 1.0
Silicon, Si 1.0
Aluminum, Al 0.2
Carbon, C 0.080
Phosphorous, P 0.040
Sulfur, S 0.030


ASTM A240 TP405 Stainless Metal Plate Physical Properties

Properties Metric Imperial
Tensile strength 448 MPa 65000 psi
Yield strength (@strain 0.200 %/) 276 MPa 40000 psi
Elastic modulus 200 GPa 29007 ksi
Poisson's ratio 0.27-0.30 0.27-0.30
Elongation at break (in 50 mm) 25.00% 25.00%
Izod Impact (@20°C/68°F) 41.0 J 30.2 ft-lb
Hardness, Brinell (converted from Rockwell B hardness) 131 131
Hardness, Knoop (converted from Rockwell B hardness) 146 146
Hardness, Rockwell B 75 75
Hardness, Vickers (converted from Rockwell B hardness) 140 140

ASTM A240 Stainless Steel 405 Sheet Mechanical Properties

Properties Metric Imperial
Density 7.80 g/cm3 0.282 lb/in³


405 Stainless Steel Plate Stock

ASTM A240 TP405 Stainless Steel 2B Finish Plate ASTM A240 TP405 Stainless Steel Cold Rolled Plates
ASTM A240 TP405 Stainless Steel 4 Finish Plate ASTM A240 TP405 Stainless Steel 2D Finish Plate
ASTM A240 TP405 Stainless Steel CR Plates ASTM A240 TP405 Stainless Steel 8 Finish Plate
ASTM A240 TP405 Stainless Steel Hot Rolled Plates Stainless Steel ASTM A240 TP405 HR Plates
ASTM A240 TP405 Stainless Steel Plates ASTM A240 TP405 Stainless Steel Chequered Plate

 

Customer Visit

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

gnee steelgnee steel

 

Hot Tags: astm a240 tp405 plate, China astm a240 tp405 plate suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS431 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Corrugated SS Roof Sheet, SS410 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry