Stainless Steel 317/317L Pipes & Tubes
video

Stainless Steel 317/317L Pipes & Tubes

SS 317/317L Pipes & Tubes are made with the help of various specifications such as types, shape, size, width, length, thickness, conditions, tolerance, applications, finish, surface, forms, and end. These pipes and tubes are made with various chemical compositions such as carbon, manganese, silicon, phosphorus, sulfur, chromium, nickel, nitrogen, and molybdenum. These pipes are made with both physical and mechanical properties such as tensile strength, yield strength, electrical conductivity, and thermal conductivity, and electrical resistivity, modulus of expansion, elongation, melting point, and density as well. These tubes are available in several forms and types such as CDW, ERW, seamless, fabricated, and welded as well.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 317/317l pipes & tubes in China. If you're going to wholesale high quality stainless steel 317/317l pipes & tubes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SS 317/317L Pipes & Tubes are made with the help of various specifications such as types, shape, size, width, length, thickness, conditions, tolerance, applications, finish, surface, forms, and end. These pipes and tubes are made with various chemical compositions such as carbon, manganese, silicon, phosphorus, sulfur, chromium, nickel, nitrogen, and molybdenum. These pipes are made with both physical and mechanical properties such as tensile strength, yield strength, electrical conductivity, and thermal conductivity, and electrical resistivity, modulus of expansion, elongation, melting point, and density as well. These tubes are available in several forms and types such as CDW, ERW, seamless, fabricated, and welded as well.

 

product-750-750product-750-750product-720-720

 

CHEMICAL COMPOSITION OF STAINLESS STEEL 317/317L SEAMLESS PIPES AND TUBES

Grade C Mn Si P S Cr Mo Ni N
317 0.08 max 2 max 1 max 0.040 max 0.03 max 18 – 20 3 – 4 11 – 14 -
317L 0.035 max 2 max 1 max 0.040 max 0.03 max 18 – 20 3 – 4 11 – 15 -

MECHANICAL PROPERTIES OF STAINLESS STEEL 317/317L SEAMLESS PIPES AND TUBES

Density 8.0 g/cm3
Melting Point 1454 °C (2650 °F)
Tensile Strength Psi – 75000 , MPa – 515
Yield Strength (0.2%Offset) Psi – 30000 , MPa – 205
Elongation 35 %

PHYSICAL PROPERTIES OF 317/317L STAINLESS STEEL PIPES AND TUBES

Physical Properties (Room Temperature)

Specific Heat (0-100°C)

500

J.kg-1.°K-1

Thermal Conductivity

14.6

W.m -1.°K-1

Thermal Expansion

16.5

mm/m/°C

Modulus Elasticity

193

GPa

Electrical Resistivity

7.4

μohm/cm

Density

7.99

g/cm3