S31803 S32205 S32750 Seamless Steel Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of s31803 s32205 s32750 seamless steel pipe in China. If you're going to wholesale high quality s31803 s32205 s32750 seamless steel pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
S31803 S32205 S32750 Seamless Steel Pipe
Description
The 2205 Duplex Stainless Pipe produced in accordance to ASTM A790 specification could be constructed by either a seamless construction or an automatic welding process. If the 22cr Duplex Pipe is to be welded, no filler metal is required to be added to the alloy during its welding process. Heat and product analysis is to be performed on the SA 789 Alloy 2205 Pipe Material. All Duplex 2205 Seamless Pipe produced according to the ASTM A789 must be furnished in a heat treated condition. This heat treatment performed on the Duplex 2205 Pipe must be keeping with accordance to the specified temperature and quench conditions. You can find out more about the 2205 Pipe Sizes and the price list on our webpage. Contact us get the best quote for Duplex 2205 Welded Pipe.
Product Description:
| Product name | Stainless steel pipe/ tube |
| Technique | Welded/ Seamless |
| Standard | ASTM A778, ASTM A312, JIS G3448, EN10312, CJ/T 151 |
| Material | Mainly: 201, 202, 304, 304L, 304H, 316, 316L, 316Ti, 2205, 330, 630, 660, 409L, 321, 310S, 410, 416, 410S, 430, 347H, 2Cr13, 3Cr13 etc 300series: 301, 302, 303, 304, 304L, 309, 309s, 310, 310S, 316, 316L, 316Ti, 317L, 321, 347 200series: 201, 202, 202cu, 204 400series: 409, 409L, 410, 420, 430, 431, 439, 440, 441, 444 Others: 2205, 2507, 2906, 330, 660, 630, 631, 17-4ph, 17-7ph, S318039 904L,etc Duplex stainless steel: S22053, S25073, S22253, S31803, S32205, S32304 Special Stainless Steel: 904L, 347/347H, 317/317L, 316Ti, 254Mo |
| Outside Diameter | Seamless Pipe: 4mm-812.80mm |
| Welded Pipe: single slit(Φ8mm-Φ630mm); girth(Φ630mm-Φ3000mm) | |
| Thickness | Seamless Pipe: 0.5mm - 60mm |
| Welded Pipe: single slit(0.5mm-25mm); girth(3mm-45mm) | |
| Length | ≤12000mm or as per customer request |
| Surface | Polishing (180#,220#,240#,320#400#,600#), Hairline, Aid Pickling, Inside weld leveling, Online bright heat) |
| Application | Decoration (Processed into railings, handrails, doors and windows), Medical, Industry, Water Supply, Municipal Engineering, etc |
| Delivery time | 7-15 days subject to the clients' requirement and quantity |
| Package | Clients' requirement and standard export sea-worthy packing |

Hot Tags: s31803 s32205 s32750 seamless steel pipe, China s31803 s32205 s32750 seamless steel pipe suppliers, 410 Stainless Steel Pipe, 1 4509 1 4510 Pipes And Tubes, Slip On Flanges, Inconel 625 Alloy Steel Plate, 420J1 420J2 316 Stainless Pipe, Stainless Steel High Pressure Pipe