ASTM A312 SMO 254 Stainless Steel Seamless Pipes
video

ASTM A312 SMO 254 Stainless Steel Seamless Pipes

SMO 254 Stainless pipe efficiently resists pitting, crevice corrosion and chloride stress corrosion cracking. 254 SMO Tubing is well known for high ductility and good impact strength. It is also known as moly 6 due to the addition of molybdenum in trace amounts. 254 SMO Pipe Suppliers recommend these pipes due to their ability to work under high temperatures and maintain high strength even under volatile conditions.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a312 smo 254 stainless steel seamless pipes in China. If you're going to wholesale high quality astm a312 smo 254 stainless steel seamless pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SMO 254 Erw Tubes have a great influencing potential and ductility at ambient and sub-zero temperatures. 1.4547 Hollow Pipe produces a weld that has better corrosion resistant properties than its parent metal due to it being over alloyed. Alloy 254 High-Pressure Tubes are stronger than common austenitic grades and are easy to weld. Din 1.4547 Welded Tubes are considered to be a cost-effective substitute for the alloy with high nickel content and titanium. To attain maximum corrosion resistant properties Tubo Smo 254 requires post-processing annealing.

seamless pipess seamless tube

 

254 SMO Properties:

  • Excellent resistance to pitting and crevice corrosion, PRE = ≥42.5%
  • High resistance to general corrosion
  • High resistance to stress corrosion cracking
  • Higher strength than conventional austenitic stainless steels
  • Good weldability

 

Chemical Composition of ASTM A312 SMO 254 Seamless Stainless Pipes

C Si Mn P S Cr Ni Mo N Cu
≤0.020 ≤0.80 ≤1.00 ≤0.030 ≤0.010 20 18 6.1 0.20 0.7

 

Mechanical Properties of ASTM A312 SMO 254 Stainless Steel Seamless Pipes

 

Properties Metric Imperial
Tensile strength 680 MPa 98600 psi
Yield strength 300 MPa 43500 psi
Modulus of elasticity 195 GPa 28300 ksi
Shear modulus 75 GPa 10900 ksi
Poisson's ratio 0.30 0.30
Elongation at break 50 % 50 %
Hardness, Brinell 210 210

 

ASTM A312 SMO 254 SS Seamless Pipes Physical Properties

 

Specific Heat (0-100°C) 500 J.kg-1.°K-1
Thermal Conductivity 14 W.m -1.°K-1
Thermal Expansion 16.5 mm/m/°C
Modulus Elasticity 196 GPa
Electrical Resistivity 8.5 μohm/cm
Density 8.0 g/cm3

 

Customer Visit

 GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

GNEE STEELGNEE STEEL

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

 

Hot Tags: astm a312 smo 254 stainless steel seamless pipes, China astm a312 smo 254 stainless steel seamless pipes suppliers, Inconel 625 Alloy Steel Plate, Stainless Steel High Pressure Pipe, 1 4509 1 4510 Pipes And Tubes, SS410 Stainless Steel Pipe, 420J1 420J2 316 Stainless Pipe, 410 Stainless Steel Pipe