ASTM A269 TP 310S High Temperature Resistant Pipes
Surface Condition:Ba, Annealing Pickling, Polished
Transport Package:Wooden Box
Specification:6 - 114.3 mm
Certificate:ISO 9001-2000,ASME,DNV
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a269 tp 310s high temperature resistant pipes in China. If you're going to wholesale high quality astm a269 tp 310s high temperature resistant pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM A269 TP 310S high temperature resistant pipe is a stainless steel pipe specially designed to work in high temperature environment.
The main material of ASTM A269 TP 310S corrosion resistant pipe is 310S stainless steel, also known as 0Cr25Ni20, which belongs to austenitic chromium-nickel stainless steel.
310S stainless steel heat exchanger tube has a high proportion of chromium (Cr) and nickel (Ni), which makes it have good oxidation resistance, corrosion resistance and high temperature resistance.
310S stainless steel pipe has a wide range of specifications, including: Outer diameter: 6mm to 940mm, wall thickness: 0.8mm to 60mm.
Products Data
Chemical Composition of ASTM A269 TP 310s Stainless Steel Pipes
| Element | Content (%) |
| Iron, Fe | 54 |
| Chromium, Cr | 24-26 |
| Nickel, Ni | 19-22 |
| Manganese, Mn | 2 |
| Silicon, Si | 1.50 |
| Carbon, C | 0.080 |
| Phosphorous, P | 0.045 |
| Sulfur, S | 0.030 |
Physical Properties of ASTM A269 TP 310s Heat Exchanger Tube
| Properties | Metric | Imperial |
| Density | 8 g/cm3 | 0.289 lb/in³ |
| Melting point | 1455°C | 2650°F |
Products Display
ASTM A269 TP310S Stainless Steel Clad Pipe

Why choosing GNEE
GNEE's main equipment includes Φ50~Φ250 series hot rolling piercing units, LG30~LG450 series cold rolling units, YLB5T~YLB1000T series high-precision hydraulic cold drawing units, large-scale casing boring units, normalizing furnaces, tempering furnaces and box furnaces, various pipe fittings production units, etc.
If you have any inquiry, please don't hesitate to contact us immediately! Free Quote ss@gneesteel.com
GNEE CUSTOMER VISIT

GNEE FACTORY ENVIRONMENT

GNEE PACKAGING AND SHIPPING

FAQ
1.how long can i get the feedback after we sent the inquiry?
we will reply you within 24 hours in working day.
2.are you a direct manufacturer or trading company?
We are a company integrating industry and trade
3.what products can you offer?
Our main products include stainless steel pipes, pipe fittings, flanges, valves, etc.
Hot Tags: astm a269 tp 310s high temperature resistant pipes, China astm a269 tp 310s high temperature resistant pipes suppliers, 1 4509 1 4510 Pipes And Tubes, Slip On Flanges, 410 Stainless Steel Pipe, 420J1 420J2 316 Stainless Pipe, Inconel 625 Alloy Steel Plate, SS410 Stainless Steel Pipe
You Might Also Like
Send Inquiry