ASTM A269 TP316L Sanitary Stainless Steel Pipes
Surface Condition:Ba, Annealing Pickling, Polished
Transport Package:Wooden Box
Specification:6 - 114.3 mm
Certificate:ISO 9001-2000,ASME,DNV
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a269 tp316l sanitary stainless steel pipes in China. If you're going to wholesale high quality astm a269 tp316l sanitary stainless steel pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM A269 TP316L sanitary stainless steel pipe is a molybdenum-containing austenitic stainless steel with excellent corrosion resistance, especially in chloride environments. With better corrosion resistance and higher nickel content than 304 stainless steel, it is suitable for a wider range of industrial applications.
ASTM A269 TP316L sanitary pipe supplied by GNEE is usually bright annealed to improve its surface finish and corrosion resistance. In addition, 316L stainless polished steel pipe has uniform wall thickness, high dimensional accuracy, and the inner surface finish reaches Ra<0.25um.
Products Data
ASTM A269 TP 316L Stainless Steel Tubing Specifications
| Standard | ASTM A269 |
|---|---|
| Grade | 316L Stainless Steel |
| Tubing Type | Welded Tubing Seamless Tubing |
| Tubing Form | Coil Tubing Straight Tubing |
| Finishes | Annealing Pickling Bright Annealing |
| Outside Diameter | 6.35 Mm To 127 Mm |
| Thickness |
0.51 Mm To 8 Mm |
ASTM A269 TP 316L Stainless Steel Capillary Pipes Chemical Composition
| Grade | C | Mn | P | S | Si | Ni | Cr | Mo |
|---|---|---|---|---|---|---|---|---|
| 316L | 0.035 | 2.00 | 0.045 | 0.030 | 1.0 | 10-14 | 16-18 | 2-3 |
ASTM A269 TP 316L High Pressure Pipe Mechanical Properties
| Grade | Tensile Strength(Mpa) | Yield Point(Mpa) | Elongation(%) | Elongation(%) |
|---|---|---|---|---|
| 316L | 485 | 170 | 35 | 25 |
Products Display
ASTM A269 TP316L Electropolished Tubing

Why choosing GNEE
GNEE has advanced production equipment, including 8 sets of hydraulic cold drawing units, LG380 large cold rolling units, fully automatic gas solution treatment furnaces, and a full set of non-destructive testing equipment such as water pressure, eddy current, and ultrasound.
The warehouse has more than 2,000 tons of stock, with complete specifications. Common specifications are shipped on the same day, and medium and large diameter stainless steel thick-walled pipes can be cut and sold.
If you have any inquiry, please don't hesitate to contact us immediately! Free Quote ss@gneesteel.com
GNEE CUSTOMER VISIT

GNEE FACTORY ENVIRONMENT

GNEE PACKAGING AND SHIPPING

FAQ
1.how long can i get the feedback after we sent the inquiry?
we will reply you within 24 hours in working day.
2.are you a direct manufacturer or trading company?
We are a company integrating industry and trade
3.what products can you offer?
Our main products include stainless steel pipes, pipe fittings, flanges, valves, etc.
Hot Tags: astm a269 tp316l sanitary stainless steel pipes, China astm a269 tp316l sanitary stainless steel pipes suppliers, Inconel 625 Alloy Steel Plate, Stainless Steel High Pressure Pipe, SS410 Stainless Steel Pipe, 1 4509 1 4510 Pipes And Tubes, 420J1 420J2 316 Stainless Pipe, 410 Stainless Steel Pipe
You Might Also Like
Send Inquiry