1.4439 Seamless Stainless Steel Tube
video

1.4439 Seamless Stainless Steel Tube

Alloy 317LMN is non-magnetic in the annealed condition. It cannot be hardened by heat treatment, only by cold working. The alloy can be easily welded and processed by standard shop fabrication practices.The nitrogen content of Alloy 317LMN acts as a strengthening agent giving it a higher yield strength than 317L .Alloy 317LMN is also a low carbon grade which enables it to be used in the as-welded condition free from chromium carbide precipitation on the grain boundaries.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4439 seamless stainless steel tube in China. If you're going to wholesale high quality 1.4439 seamless stainless steel tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

1.4439 Seamless Stainless Steel Tube

1.4439 is a German standard austenitic stainless steel, also known as X2CrNiMoN17-13-5. Below is comprehensive information about this stainless steel.

Base data:

- Density: 7.9g/cm³

- Melting point: 1400℃

- Magnetic: non-magnetic

- Modulus of elasticity: 200 GPa

- Tensile strength: 750-1000 MPa

- Yield strength: 450-600 MPa

- Elongation: >25%

introduce:

1.4439 is a high alloy content stainless steel with excellent corrosion resistance and mechanical strength. It has good resistance to acid, salt water and chloride ion corrosion, and is especially suitable for working conditions in acidic environments. In addition, this stainless steel also has good heat resistance at high temperatures.

advantage:

- Corrosion resistance: It has excellent resistance to acid, salt water and chloride ion corrosion, and can maintain stability for a long time in corrosive environments.

- Good mechanical strength: It has high tensile strength and yield strength and can withstand certain mechanical loads.

- High temperature resistance: It has good heat resistance in high temperature environments and is not prone to deformation or cracking.

use:

- Chemical industry: suitable for chemical pipelines, containers, reactors, etc., able to withstand the effects of various corrosive media.

- Marine engineering: In the marine environment, it can withstand the corrosion of salt water and seawater, and is used to manufacture equipment such as offshore platforms and marine pipelines.

- Food processing: Due to its acid resistance, it is suitable for use in food processing equipment, pharmaceutical equipment, etc.

Element:

- Carbon (C): ≤0.03%

- Silicon (Si): ≤1.00%

- Manganese (Mn): ≤2.00%

- Phosphorus (P): ≤0.040%

- Sulfur (S): ≤0.015%

- Nickel (Ni): 12.5-15.0%

- Chromium (Cr): 17.0-19.0%

- Molybdenum (Mo): 4.0-5.0%

- Nitrogen (N): 0.12-0.22%