Stainless Steel Coil 316L
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel coil 316l in China. If you're going to wholesale high quality stainless steel coil 316l made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
316L has a wide range of applications in the chemical industry because of its excellent corrosion resistance. 316L is also a derivative of 18-8 austenitic stainless steel, with 2 ~ 3% Mo element added.




On the basis of 316L, many kinds of steel are also derived. For example, 316Ti is derived after adding a small amount of Ti, 316N is derived after adding a small amount of N, and 317L is derived by increasing the content of Ni and Mo.
Most of the existing 316L in the market are produced according to American standards.
For cost consideration, steel mills generally put the Ni content of products as far as possible by the lower limit.
The American standard stipulates that the Ni content of 316L is 10 ~ 14%, while the Japanese standard stipulates that the Ni content of 316L is 12 ~ 15%.
According to the minimum standard, there is a 2% difference between the American standard and Japanese standard in the Ni content, which is still quite huge in the price. Therefore, customers still need to see clearly when buying 316L products, whether the products refer to ASTM or JIS standards.
The Mo content of 316L makes the steel have excellent pitting resistance and can be safely used in environments containing Cl- and other halogen ions.
Because 316L is mainly used for its chemical properties, steel mills have slightly lower requirements for surface inspection of 316L (relative to 304), and customers with higher surface requirements should strengthen surface inspection.
| Grade | Euronorm | China GB | Japanese JIS | |
| No. | ||||
| 316L | 1.4404 | 022Cr17Ni12Mo2 | SUS316L | |
Stainless Steel 316L Chemical Comppsition :
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 316L | Min. Max. |
≤0.03 | ≤2.00 | ≤1.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 2.00~3.00 | 10.00~14.00 | |
Tensile strength σb (MPa) : ≥480
Conditional yield strength σ0.2 (MPa) : ≥177
Elongation Δ5 (%) : ≥40
Section shrinkage ψ(%) : ≥60
Hardness: 187 hb or less;
90 HRB or less;
200 hv or less
Density: 7.98g/cm3;
Specific heat capacity ratio (20℃) : 0.502J/(g*K)
FAQ
Q: How long is your delivery time?
A: It is according to quantity. Generally it is 30 days.
Q: Can you provide us sample, is it free or need to pay?
A: If you don't need to print your logo or other artwork on the products, we will not charge any cost, just tell us your freight collect account like Fedex, DHL, TNT. If you don't have, we need to charge Express fee properly.
Q: Can I get your best price?
A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.
Hot Tags: stainless steel coil 316l, China stainless steel coil 316l suppliers, 2507 Stainless Steel Coil, 304 316 316l SS Cold Rolled Steel Coils, 316L Stainless Steel Coil, AISI430 Stainless Steel Foil
Previous
321 304 316 SS CoilYou Might Also Like
Send Inquiry