Stainless Steel Coil 201
video

Stainless Steel Coil 201

The 200 series stainless steel was first developed in the United States during World War II as a substitute for the 300 series stainless steel. At that time, because of the war, nickel as a strategic material was strictly controlled by the countries concerned, and the supply of nickel in the United States was seriously short.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel coil 201 in China. If you're going to wholesale high quality stainless steel coil 201 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

 

 

The 200 series stainless steel was first developed in the United States during World War II as a substitute for the 300 series stainless steel.

At that time, because of the war, nickel as a strategic material was strictly controlled by the countries concerned, and the supply of nickel in the United States was seriously short.

 

product-750-750product-750-750product-750-750product-750-750

 

This new series of austenitic stainless steels with manganese instead of nickel was developed in the United States in order to solve the problem of production and supply of stainless steel under the condition of severe nickel shortage.

After the end of World War II, the supply of nickel in the United States gradually improved, so the production of 300 series stainless steel is no longer restricted by raw material constraints, so the 200 series did not get a big development.

Several original participation in the development of 200 series of stainless steel Indians, after returning to India, from India is a relatively rich in manganese resources, nickel resources lack of national conditions, will be developed in the United States 200 series of stainless steel varieties back to India.

The success of the 200 series stainless steel in India is due to the possibility of replacing 304 stainless steel in some specific applications.

Most of the 200 series stainless steels sold in the Chinese market have little control on sulfur and carbon content according to national standards, and use manganese (and nitrogen) to replace part or all of nickel to produce austenitic stainless steels with lower nickel content.

The disadvantage of this series of materials is: below 18% chromium content and low nickel content can not reach balance and form ferrite, for this reason, 200 series of stainless steel chromium content to 13.5% ~ 15%, in some cases down to 13% ~ 14%, its corrosion resistance is not compared with 304 and other similar steels.

In addition, manganese and, in some cases, copper reduce the effect of re-passivation under acidic conditions common in the corrosion sites of deposits and crevasses.

The destruction rate of 200 series steels under these conditions is approximately 10-100 times that of 304 stainless steels.

The residual sulfur and carbon content of these steels is often not controlled during production, and the material cannot be traced to its source, even when it is recycled.

If Cr-Mn steels are not specified, they can become a dangerous scrap mix, resulting in castings containing unexpectedly high levels of manganese.

This is the most cost effective grade of steel. So the 201 Stainless Steel coil Price is lower compared to other grades of stainless steels and all metallic products in general. There are different versions of the material with low carbon and high carbon content. The low carbon version, 201 coils are very good for welding applications as they have less carbide precipitation and less localized corrosion.

 

Grade Euronorm China GB Japanese JIS
No.
201 1.4372 12Cr17Mn6Ni5N SUS201

 

Stainless Steel 201 Chemical Comppsition :

Grade C Mn Si P S Cr Mo Ni N
201 Min.
Max.
≤0.15 5.5~7.50 ≤1.00 ≤0.060 ≤0.03 16.0~18.0 / 3.5-5.5 ≤0.25

 

Tensile strength :520MPa

Yield strength :275MPa

Elongation :55 to 60%

Elastic modulus :29,000,000 psi is equivalent to: 203000MPa

Hardness requirement (Brinell hardness)

183 n/was (MPa).

Density :.280 LBS /cubic inch(density 7.93g/cm3)

 

FAQ

Q: How long is your delivery time?
A: It is according to quantity. Generally it is 30 days.

 

Q: Can you provide us sample, is it free or need to pay?
A: If you don't need to print your logo or other artwork on the products, we will not charge any cost, just tell us your freight collect account like Fedex, DHL, TNT. If you don't have, we need to charge Express fee properly.

 

Q: Can I get your best price?

A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.

 

Hot Tags: stainless steel coil 201, China stainless steel coil 201 suppliers, 304 316 316l SS Cold Rolled Steel Coils, AISI430 Stainless Steel Foil, 316L Stainless Steel Coil, 2507 Stainless Steel Coil

Send Inquiry

whatsapp

Phone

E-mail

Inquiry