316 Stainless Steel Coil
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 316 stainless steel coil in China. If you're going to wholesale high quality 316 stainless steel coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
316 stainless steel because of the addition of Mo element, so that its corrosion resistance, and high temperature strength has been greatly improved, high temperature resistance can reach 1200-1300 degrees, can be used under harsh conditions.
Application: Seawater equipment, chemical, dye, paper making, oxalic acid, fertilizer and other production equipment;
Photographs, food industry, coastal facilities, ropes, CD rods, bolts, nuts.




316 stainless steel because of the addition of Mo element, so that its corrosion resistance, and high temperature strength has been greatly improved, high temperature resistance can reach 1200-1300 degrees, can be used under harsh conditions.
Application: Seawater equipment, chemical, dye, paper making, oxalic acid, fertilizer and other production equipment;
Photographs, food industry, coastal facilities, ropes, CD rods, bolts, nuts.
Characteristics: Because of the addition of Mo, it has good corrosion resistance, atmospheric corrosion resistance and high temperature strength, which can be used under harsh conditions;
Excellent work hardening (non-magnetic);
Excellent high temperature strength;
The solid solution state is not magnetic;
Cold rolled product appearance gloss is good, beautiful;
Relative to 304 stainless steel, the price is higher.
316 stainless steel because of the addition of Mo element, so that its corrosion resistance, and high temperature strength has been greatly improved, high temperature resistance can reach 1200-1300 degrees, can be used under harsh conditions.
Application: Seawater equipment, chemical, dye, paper making, oxalic acid, fertilizer and other production equipment;
Photographs, food industry, coastal facilities, ropes, CD rods, bolts, nuts.
| Grade | Euronorm | China GB | Japanese JIS | |
| No. | ||||
| 316 | 1.4401 | 0Cr17Ni12Mo2 | SUS316 | |
Stainless Steel 316 Chemical Comppsition :
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 316 | Min. Max. |
≤0.08 | ≤2.00 | ≤1.00 | ≤0.035 | ≤0.03 | 16.0-18.5 | 2.0-3.0 | 10.0-14.0 | |
The tensile strength (MPa) was 620 MIN
The yield strength (MPa) was 310 MIN
Elongation rate (%) 30 MIN
Area reduction (%) 40 MIN
FAQ
Q: How long is your delivery time?
A: It is according to quantity. Generally it is 30 days.
Q: Can you provide us sample, is it free or need to pay?
A: If you don't need to print your logo or other artwork on the products, we will not charge any cost, just tell us your freight collect account like Fedex, DHL, TNT. If you don't have, we need to charge Express fee properly.
Q: Can I get your best price?
A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.
Hot Tags: 316 stainless steel coil, China 316 stainless steel coil suppliers, 316L Stainless Steel Coil, 2507 Stainless Steel Coil, 304 316 316l SS Cold Rolled Steel Coils, AISI430 Stainless Steel Foil