Class400 Steel Plate 6.0*2000*6000mm Drilling AR400 Steel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of class400 steel plate 6.0*2000*6000mm drilling ar400 steel plate in China. If you're going to wholesale high quality class400 steel plate 6.0*2000*6000mm drilling ar400 steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Class400 Steel Plate 6.0*2000*6000mm Drilling AR400 Steel Plate
Description
| Grade: | NM400 Class400 | Thickness: | 3-100mm |
|---|---|---|---|
| Standard: | ASTM, AISI, DIN, EN, GB, JIS | Width: | 1000-2000mm |
| Technique: | Cold Rolled Hot Rolled | Length: | As Per Customers' Requiremen |
| High Light: |
stainless steel plate,stainless steel metal sheet |
||
Class400 Steel Plate 6.0*2000*6000mm Drilling AR400 Steel Plate
NM400 is a high-strength wear-resistant steel. NM400 has a very high mechanical strength; the mechanical properties of the common low-alloy steel plate 3 times to 5 times times; can significantly improve the wear resistance of associated components; thus improving the service life of the machine; reducing production costs. the product surface hardness is usually 360~450HB. Used in mining and construction machinery wear wearing parts machining and manufacturing application of structural steel.
NM400 is a kind of wear-resistant steel. NM-wear-resistant purpose of "resistance" and "grinding" first letters 400 Brinell hardness value of Hanyu Pinyin HB values. (400 hardness values in a broad sense, NM400 hardness range 360-420. )
Key words: Wear Plate,Wear-Resisting Plate,Wear Resistant Plate,Abrasion-Resistant Plate,Anti-Friction Plate.
Thickness: 6mm to60mm
Width: 1450mm to 2500mm,
Length: 3000mm to 10000mm
Any size is no problems. We can cut our plates for you.
More informations of our products
| Products | Abrasion Resistant steel plate / Wear Resistant Steel Plate |
| Thickness | ≥6mm |
| Width | 1.5~2.5m depend on requirement |
| Length | cut to size according to your requirements |
| Grade | 400 / 450 / 500 / 600 |
| NM360 / NM400 / NM450 / NM500 / NR360 / NR400 / B-HARD360 / B-HARD400 / B-HARD450 / KN-55 / KN-60 / KN-63 | |
| XAR400 / XAR450 / XAR500 / XAR600 / Dillidur400 / Dillidur500 | |
| QUARD400 / QUARD450 / QUARD500 | |
| Payment term | T/T, West Union, Escrow, L/C at sight |
| Tolerance | Comply with standard or requirements |
| Heat Treatment | Hot rolled, Annealing, Tempered |
| Packing | Standard exporting packing or as requirements |
| Certificate | ISO SGS BV |
| Application | Widely used in petroleum industry, chemical industry, power station, boiler with making equipments or hardware like reactor, heat exchanger, seperator, sphere, liquid gas storage tank, nuclear-power reacto,pressure vessel, boiler drum, liquified petroleum gas pot, volute and so on. |
Chemical of composition
| Grade | C | Si | Mn | P | S | Cr | Ni | Mo | B |
| NM360 | ≤0.17 | ≤0.50 | ≤1.50 | ≤0.025 | ≤0.015 | ≤0.70 | ≤0.50 | ≤0.40 | ≤0.005 |
| NM400 | ≤0.24 | ≤0.50 | ≤1.60 | ≤0.025 | ≤0.015 | 0.40-0.80 | 0.20-0.50 | 0.20-0.50 | ≤0.005 |
| NM450 | ≤0.26 | ≤0.50 | ≤1.60 | ≤0.025 | ≤0.015 | ≤1.50 | ≤1.00 | ≤0.50 | ≤0.004 |
| NM500 | ≤0.38 | ≤0.50 | ≤1.70 | ≤0.020 | ≤0.010 | ≤1.20 | ≤1.00 | ≤0.65 | 0.005-0.006 |
| 400 | ≤0.22 | ≤0.70 | ≤1.60 | ≤0.025 | ≤0.015 | ≤0.80 | ≤0.50 | ≤0.25 | ≤0.004 |
| 450 | ≤0.25 | ≤0.70 | ≤1.60 | ≤0.025 | ≤0.010 | ≤0.50 | ≤0.25 | ≤0.25 | ≤0.004 |
| 500 | ≤0.29 | ≤0.70 | ≤1.60 | ≤0.025 | ≤0.015 | ≤1.00 | ≤1.00 | ≤0.60 | ≤0.004 |
| Grade | Yield strength/MPa | Tensile Strength /MPa | Elongation A50/% | Hardness HBW10/3000 | Impact /J(-20°C) | 90°Cold bending |
| NM360 | 900 | 1050 | 12 | 320-390 | 21 | ≥3a |
| NM400 | 950 | 1200 | 12 | 380-430 | 21 | D≥3a |
| NM450 | 1050 | 1250 | 7 | 420-480 | 21 | D≥4.5a |
| NM500 | 1100 | 1350 | 6 | 470 | 17 | D≥6a |
| NM550 | - | - | - | 530 | - | D≥6a |
Features
Excellent Cold Bending & Welding Properties
Through Hardened for Long Wear Life
Flat Clean, Shot Blasted and Primed Finished Products
High Impact Properties
Grain-Refinen
FAQ:
Q1.Are you factory or trading company?
A1. We had our own cooperate fatory with good cooperation and long time(5 years) establish business .
Q2.How long have you been in this product?
A2:More than 8 years.
Q3. What's the minium quantity(MOQ)?
A3. 20 Metric tons
Q4. How long is shipping time?
A4. 7 (ready-made products)-10days(OEM)


Hot Tags: class400 steel plate 6.0*2000*6000mm drilling ar400 steel plate, China class400 steel plate 6.0*2000*6000mm drilling ar400 steel plate suppliers, 304 316 316l SS Cold Rolled Steel Coils, AISI430 Stainless Steel Foil, 2507 Stainless Steel Coil, 316L Stainless Steel Coil