Cold Rolled Stainless Steel 316L Coil Slit Edge
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of cold rolled stainless steel 316l coil slit edge in China. If you're going to wholesale high quality cold rolled stainless steel 316l coil slit edge made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Cold Rolled Stainless Steel 316L Coil Slit Edge
STAINLESS STEEL COIL/PLATE
1. Specifications about Coil
| ITEM | Stainless Steel coil |
| Brand | RONSCO,BAOSTEEL, JISCO, TISCO, etc. |
| Grade |
201.202.301.302.304.304L.310S.316.316L.321.430.430A.309S.2205.2507.2520.430.630.631 .410.440.904Lect. Or Customized |
| Certificate |
SGS,BV,IQI,TUV,ISO,etc |
| Length |
As Customer requirements |
| Surface | No.1, 2B, BA, 8K Mirror, Hairline,satin, Embossed,brush,No.4,HL,matt,pvc film,laser film. |
| Standard | GB, AISI, ASTM, ASME, EN, BS, DIN, JIS |
| Package | Standard export sea-worthy packing or customized |
| MOQ | 5 Ton |