Stainless Steel 321 Coil
video

Stainless Steel 321 Coil

321 stainless steel is a titanium-stabilized austenitic stainless steel with excellent resistance to intergranular corrosion, good overall corrosion resistance, and high temperature strength. It is particularly useful for applications that involve continuous and intermittent heating within the carbide precipitation range of 427-816°C (800-1500°F).
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 321 coil in China. If you're going to wholesale high quality stainless steel 321 coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

321 stainless steel is a titanium-stabilized austenitic stainless steel with excellent resistance to intergranular corrosion, good overall corrosion resistance, and high temperature strength. It is particularly useful for applications that involve continuous and intermittent heating within the carbide precipitation range of 427-816°C (800-1500°F).

4 93

Attribute Description
Product Name 321 Stainless Steel Coil
Standards ASTM A240, ASTM A666, UNS S32100
Thickness Range 0.3 mm to 6.0 mm
Width Up to 1500 mm
Length Custom lengths available
Surface Finish 2B, BA, No. 1, No. 4, HL, Mirror, or custom finishes

4 174

Intergranular Corrosion Resistance: Superior resistance to intergranular corrosion, especially after exposure to temperatures in the chromium carbide precipitation range.

High Temperature Strength: Maintains strength and corrosion resistance at high temperatures up to 816°C (1500°F).

Good Formability: Easily fabricated with good ductility, suitable for deep drawing and bending.

Versatility: Suitable for a wide range of applications across different industries.

Stabilized by Titanium: Titanium addition minimizes carbide precipitation during welding, enhancing weldability.

 