Hot Dip Galvanized Coil Galvanized Coil

The first and foremost method for galvanization is hot-dip galvanizing. The process is very similar to what the name suggests! In this method, steel or iron is dipped in a molten pool of zinc that maintains a temperature of around 860°F (460 °C). This molten bath begins a metallurgical bond between the zinc and the receiving metal. After the metal is pulled from the bath, it reacts to being exposed to the atmosphere, and the pure zinc mixes with oxygen to form zinc oxide. The zinc-oxide further reacts to carbon dioxide and forms zinc carbonate, which makes up the final protective coating on the material. The tell-tale sign of a hot-dipped galvanized material is the presence of a crystalline-like pattern on the surface, sometimes referred to as “spangle.”
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hot dip galvanized coil galvanized coil in China. If you're going to wholesale high quality hot dip galvanized coil galvanized coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Plating definition

(1)Normal spangle coating
(2)minimized spangle coating
(3)Spangle-free coating
(4) zinc-iron alloy coating
The steel strip after passing through the galvanizing bath is heat treated so that the entire coating forms an alloy layer of zinc and iron. This coating has a dark gray appearance with no metallic luster and is easily powdered during the violent forming process. It is suitable for use in addition to general A coating that can be painted directly without further processing other than cleaning.
(5) Differential coating differential coating
For both sides of the galvanized steel sheet, coatings with different zinc layer weights are required.
(6)Skin pass
Finishing is a cold rolling process with slight deformation on galvanized steel sheets for one or more of the following purposes.
Improve the surface appearance of galvanized steel sheets or be suitable for decorative coatings; temporarily minimize the slip lines (Lüders lines) or creases produced during processing of finished products, etc.

Defect
Mainly include: falling off, scratches, passivation spots, zinc particles, thick edges, air knife streaks, air knife scratches, exposed steel, inclusions, mechanical damage, poor steel base performance, wavy edges, curved edges, inappropriate size, Imprinting, inconsistent zinc layer thickness, roller printing, etc.
The main reasons for the zinc layer to fall off are: surface oxidation, silicon compounds, cold rolling emulsion is too dirty, NOF section oxidation atmosphere and protective gas dew point is too high, unreasonable air-fuel ratio, low hydrogen flow, oxygen penetration into the furnace, strip steel The temperature of entering the pot is low, the furnace pressure in the RWP section is low and the furnace door sucks air, the furnace temperature in the NOF section is low, the grease cannot be completely evaporated, the aluminum content of the zinc pot is low, the unit speed is too fast, the reduction is insufficient, and the zinc liquid remains The time is too short and the coating is too thick.

CRGO Grain Oriented Electrical SteelCRGO Grain Oriented Electrical Steel

product-1500-1500

product-500-500

 

FAQ

Q: Can you provide sample?

A: Yes, for regular sizes sample is free but buyer need to pay freight cost.

Q:How can I get a quotation from you?

A:You can leave us message, and we will reply every message in time. Or we may talk on line by trade manager. And you can also find our contact information on contact page.

Q: Do you accept the third party inspection?

A: Yes absolutely we accept.

Q:About product prices?

A:Prices vary from period to period due to cyclical changes in the price of raw materials.

Q: Can I get your best price?

A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.