Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of aisi 316l cold rolled stainless steel strips sus316l ba finish bright in China. If you're going to wholesale high quality aisi 316l cold rolled stainless steel strips sus316l ba finish bright made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
AISI 316L Cold Rolled Stainless Steel Strip SUS316L Stainless Steel Banding BA Finish Bright
Description:
Standard:ASTM A240,GB/T 4237, GB/T 8165, BS 1449, DIN17460, DIN 17441
Grade:300series
Thickness:0.05mm-0.50mm
Width:4.0mm-600mm
Length:Coil
Surface finish:2B, BA, 8K, 6K, Mirror Finished,No4,
Manufacture technology:cold drawn/cold rolled/hot rolled
Applications:
1 Kitchenware: tableware, cookware, Stoves…
2 Food packing: storage cans, food containers…
3 Construction: bridge, roofing, wall, decoration, bathroom accessories…
4 Precision instruments: electrical products, aerospace…
5 Others: automotive parts, machine building, chemical processing, farming…
Specifications:
| 1. Product Name | ASTM AISI 316L stainless steel Strips |
| 2. Standard | ASTM, GB, DN,JIS,AISI |
| 3. Width | 4.0-600mm |
| 4. Length | make to order |
| 5. Thickness | 0.05-0.50mm |
| 6. Superiority | High quality and Competitive price |
| 7. Third part inspection | Third part inspection is supported by us |
| 8. Application | Decoration industry, construction field, ships building industry, food industry |
| 9. Packing | seaworthy wooden packing or as your requirement |
| 10. Delivery time | 7 days after receiving 30% deposit by T/T |
| 11. Payment terms | 30% T/T in advance, 70%T/T after the copy of B/L or 30% T/T in advance, 70% L/C at sight |
| 12. Attention | we will supply you good quality and bottom price and first-class service in china and hope to be your golden supplier. |
Chemical Composition
| C | Si | Mn | P | S | Ni | Cr | |
| 201 | 0.10Max | 1.0Max | 7.5-10.0 | 0.06Max | 0.03Max | 1.0 | 16.0-18.0 |
| 202 | 0.15Max | 1.0Max | 7.5-10.0 | 0.06Max | 0.03Max | 4.0 | 17.0-19.0 |
| 301 | 0.15Max | 1.0Max | 2.0Max | 0.065Max | 0.03Max | 6.0 | 16.0-18.0 |
| 304 | 0.07Max | 1.0Max | 2.0Max | 0.035Max | 0.03Max | 8.0 | 17.0-19.0 |
| 304L | 0.03Max | 1.0Max | 2.0Max | 0.035Max | 0.03Max | 8.0 | 18.0-20.0 |
| 316 | 0.08Max | 1.0Max | 2.0Max | 0.035Max | 0.03Max | 10.0 | 16.0-18.0 |
| 316L | 0.03Max | 1.0Max | 2.0Max | 0.035Max | 0.03Max | 10.0 | 16.0-18.0 |
| 321 | 0.12Max | 1.0Max | 2.0Max | 0.035Max | 0.03Max | 9.0 | 17.0-19.0 |
| 309S | 0.08Max | 1.0Max | 2.0Max | 0.035Max | 0.03Max | 12.0 | 22.0-24.0 |
| 310S | 0.08Max | 1.0Max | 2.0Max | 0.035Max | 0.03Max | 19.0 | 24.0-26.0 |
| Surface | Definition | Application |
| 2B |
Those finished, after cold rolling, by heat treatment,pickling or other equivalent treatment and lastly by cold rolling to given appropriate luster. |
Medical equipment, Food industry, Construction material, Kitchen utensils. |
| BA |
Those processed with bright heat treatment after cold rolling. |
Kitchen utensils, Electric equipment, Building construction. |
| NO.4 |
Those finished by polishing with No.150 to No.180 abrasives specified in JIS R6001. |
Kitchen utensils, Building construction, Medical equipment. |
| HL |
Those finished polishing so as to give continuous polishing streaks by using abrasive of suitable grain size. |
Building Construction. |
| NO.1 |
The surface finished by heat treatment and pickling or processes corresponding there to after hot rolling. |
Chemical tank, pipe
|
Applications:
1 Kitchenware: tableware, cookware, Stoves…
2 Food packing: storage cans, food containers…
3 Construction: bridge, roofing, wall, decoration, bathroom accessories…
4 Precision instruments: electrical products, aerospace…
5 Others: automotive parts, machine building, chemical processing, farming…
Additional information
Standard export seaworthy packing (with waterproof paper, metal belt pack sheet, then put them in
wooden pallet, then put in container) or customerized.
Grate car is taken to avoid any damage which might be caused during storage or transportation.
In addition, clear labels are tagged on the outside of the packages for easy identification of the product
I.D. and quality information.