Silicon Steel Coil
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of silicon steel coil in China. If you're going to wholesale high quality silicon steel coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Silicon alloy steel with a silicon content of 1.0 to 4.5% and a carbon content of less than 0.08% is called silicon steel. It has the characteristics of high magnetic permeability, low coercivity, and large resistivity, so hysteresis loss and eddy current loss are small. It is mainly used as magnetic material in motors, transformers, electrical appliances and electrical instruments. In order to meet the needs of punching and shearing processing in the manufacture of electrical appliances, a certain degree of plasticity is also required. In order to improve the magnetic induction performance and reduce the hysteresis loss, it is required that the content of harmful impurities is as low as possible, and the plate shape is required to be flat and the surface quality is good.
Oriented Silicon Steel Coil

Product parameters
| Category | Silicon content/% | Thickness/mm | Application | ||
|
Hot rolled silicon steels (non-oriented) |
Hot rolled low silicon steels (motor steels) | 1.0~2.5 | 0.5 | Household Motors and Micromotors | |
| Hot rolled high silicon steels (transformer steels) | 3.0~4.5 | 0.35,0.50 | transformer | ||
| Cold Rolled Electrical Steels | Cold-rolled non-oriented electrical steels (motor steels) | Low carbon electrical steels | ≤0.5 | 0.50,0.65 | Household motors, micro motors, small transformers and ballasts |
| Silicon steels | >0.5~3.5 | 0.35,0.50 | Medium and large electric motors/generators/transformers | ||
| Cold-rolled grain-oriented silicon steels (transformer steels) | general orientation | 2.9~3.3 | 0.18,0.23,0.27,0.30,0.35 | Large/medium and small transformers ballasts | |
| High Magnetic Orientation | |||||
| Special purpose silicon steels:Cold-rolled grain-oriented silicon steels strip | 2.9~3.3 | 0.03,0.05,0.10 | Pulse Transformers, Magnetic Amplifiers, High Frequency Transformers, Electric Welders | ||
| Cold rolled non-oriented silicon steels strip | 3.0 | 0.15,0.20 | High frequency motors and generators | ||
| Cold-rolled non-oriented silicon steels for magnetic switches | 3.0 | 0.70 | Relays and Magnetic Switches | ||
| Cold rolled high silicon steels | 6.5 | 0.1~0.5 | High frequency motors, transformers and magnetic shielding | ||
Cold Rolled Silicon Steel Coil Features
The magnetic induction of silicon steels is high, the excitation current of the iron core is reduced, and the electric energy is also saved. The high magnetic induction of silicon steels can make the maximum magnetic induction (Bm) of the design high, the iron core is small in size and light in weight, saving silicon steel, wires, insulating materials and structural materials, etc., which not only reduces the loss and manufacturing cost of the motor and transformer, but also facilitates assembly and transport. The motor, which is stacked with toothed circular punches to form an iron core, works in a running state. The silicon steels plate is required to be magnetically isotropic and made of non-oriented silicon steels. The transformer, which consists of strips stacked into an iron core or strips wound into an iron core, works in a static state and is made of cold-rolled oriented silicon steels with large magnetic anisotropy. In addition, silicon steels is required to have good punching and shearing properties, smooth surface and uniform thickness, good insulating film and small magnetic aging.
Grain Oriented Silicon Steel Coil

Hot Tags: silicon steel coil, China silicon steel coil suppliers, CRNGO Electrical Steel Coil
You Might Also Like
Send Inquiry