Cold Rolled Oriented Silicon Steel
video

Cold Rolled Oriented Silicon Steel

Electrical steel, also known as silicon steel or lamination steel, is a specific kind of steel made to have excellent magnetic properties. It is useful for a variety of electromagnetic applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of cold rolled oriented silicon steel in China. If you're going to wholesale high quality cold rolled oriented silicon steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

The main purpose of cold-rolled oriented silicon steel strip is for transformer manufacturing, so it is also called cold-rolled transformer silicon steel. Compared with cold-rolled non-oriented silicon steel, oriented silicon steel has strong magnetic directionality; it has superior high magnetic permeability and low loss characteristics in the rolling direction of easy magnetization. The iron loss of the oriented steel strip in the rolling direction is only 1/3 of the transverse direction, the magnetic permeability ratio is 6:1, and the iron loss is about 1/2 of the hot rolled strip, and the magnetic permeability is 2.5 times of the latter .

 

High magnetic induction cold-rolled silicon steel strips are all single-oriented steel strips, which are mainly used in the manufacture of electromagnetic components such as transformers and chokes in the telecommunication and instrument industries. There are two main characteristics of its application. One is that under the condition of low current, that is, weak magnetic field, the material is required to have high magnetic properties in the range of weak magnetic field, that is, high μ0 value and high B value; the second feature is the frequency of use High, usually above 400Hz, even up to 2MHz. In order to reduce the eddy current loss and the effective permeability under an alternating magnetic field, a thin strip of 0.05-0.20mm is generally used.

Product Name

Electrical Steel, Lamination Steel, Silicon Electrical Steel, Silicon Steel, Relay Steel, Transformer Steel

Category

Grain-Oriented Electrical Steel; Non-oriented electrical steel

Standard

AISI, ASTM, BS, DIN, GB, JIS, EN

Thickness

0.2- 0.8 mm

Width

900-1230 mm

Brand

GNEE

Origin

China

Packing

Export standard package (as per requirements)

Payment Terms

30% T/T in advance as deposit,70% balance against the B/L copy or 100% irrevocable L/C at sight

MOQ

3 tons per size

Delivery time

15-40 days after receiving L/C or deposit

Loading Port

China (any port in China )

Remark

Specific requirement of alloy grade,temper or specification can be discussed at your request

Oriented Electrical Steel

Oriented Silicon Steel

Grain Oriented Silicon Steel  Application

Electrical steel (silicon steel sheet) is mainly divided into two categories: grain-oriented electrical steel and grain non-oriented electrical steel.

The direction of easy magnetization grains of oriented electrical steel is distributed along the rolling direction. The rolling direction has excellent characteristics such as high magnetic induction, low iron loss and low magnetostriction. At the same time, it can also be processed by magnetic domain refinement technology to obtain lower iron Loss of performance, widely used in the field of transformer industry.

The grain non-oriented electrical steel is randomly distributed, and the electromagnetic properties are uniform in all directions. It is widely used in the motor industry.

Grain oriented electrical steel use

product-704-372

 

Hot Tags: cold rolled oriented silicon steel, China cold rolled oriented silicon steel suppliers, CRNGO Electrical Steel Coil