M15 M19 Silicon Steel Coil
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of m15 m19 silicon steel coil in China. If you're going to wholesale high quality m15 m19 silicon steel coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Electrical steel, also called lamination steel, silicon electrical steel, silicon steel or transformer steel, is a material used to produce certain magnetic cores, such as stators and rotors in transformers and motors. Electrical steel is also an indispensable material for the power, electronics and military industries.
Non-oriented electrical steel usually contains a level of 2%-3.5% silicon. It has similar magnetic properties in all directions, the so-called isotropy. Grain-oriented electrical steel usually contains a level of 3% silicon and is processed in a way to develop ideal properties in the rolling direction. Cold-rolled non-grain-oriented steel (CRNGO) is less expensive than cold-rolled grain-oriented steel (CRGO). CRNGO can be used in cost-oriented applications with the inconstant direction of magnetic flux, such as electric motors and generators. CRGO is usually in coil form and has to be cut into laminations further, being used in transformer core applications, such as certain internal parts in audio output transformers.
Technical Parameters of silicon steels
|
Thickness |
Trademark |
Theoretical density (Kg/dm2) |
Iron loss(W/Kg ) |
Magnetic induction (T) |
||||
|
50Hz |
60Hz |
|||||||
|
1.0T |
1.5T |
1.0T |
1.5T |
2500A /m |
5000A /m |
|||
|
0.35 |
35W250 |
7.60 |
0.91 |
2.26 |
1.15 |
2.85 |
1.58 |
1.67 |
|
35W270 |
1.00 |
2.40 |
1.26 |
3.05 |
1.58 |
1.67 |
||
|
35W300 |
7.65 |
1.12 |
2.65 |
1.40 |
3.30 |
1.58 |
1.67 |
|
|
35W360 |
1.24 |
2.75 |
1.54 |
3.40 |
1.59 |
1.68 |
||
|
35W400 |
1.40 |
3.18 |
1.75 |
3.95 |
1.59 |
1.67 |
||
|
35W440 |
7.70 |
1.70 |
3.75 |
2.10 |
4.70 |
1.58 |
1.67 |
|
|
0.50 |
50W270 |
7.60 |
0.98 |
2.40 |
1.27 |
3.05 |
1.58 |
1.67 |
|
50W290 |
1.10 |
2.60 |
1.43 |
3.35 |
1.58 |
1.67 |
||
|
50W310 |
7.65 |
1.22 |
2.83 |
1.57 |
3.60 |
1.58 |
1.67 |
|
|
50W350 |
1.26 |
2.91 |
1.60 |
3.70 |
1.58 |
1.67 |
||
|
50W400 |
1.45 |
3.30 |
1.83 |
4.15 |
1.59 |
1.67 |
||
|
50W470 |
7.70 |
1.63 |
3.57 |
2.05 |
4.50 |
1.59 |
1.67 |
|
|
50W600 |
7.75 |
1.90 |
4.20 |
2.40 |
5.25 |
1.59 |
1.68 |
|
Non Grain Oriented Silicon Steel Coil

Non Oriented Silicon Steel Coil Features of Silicon Steel
Great Electromagnetic Performance
The silicon steels comes with low iron loss and high magnetic induction, especially HiB steel which has lower iron loss and higher magnetic induction.
Good Shape
The material is often made in strips. Slight longitudinal and transverse thickness difference ensures a high lamination factor.
Insulating Coating
Uniform color, excellent insulative, high adhesion strength, high heat resistance, excellent processability, and superior corrosion resistance. Our silicon steels sheets is available in multiple insulating coating options, which have been reaching and RoHS certified that harmful matter content complies with domestic and overseas regulations on environmental protection.
Excellent Processability
Accessible to die-cut, with high dimensional accuracy.
Surface Quality
Our silicon steels features a smooth surface, without defects such as rust, rolling marks, holes, cold-lap,folds, bubbles, etc.
Grain Oriented Electrical Steel Coil Application
Silicon steels is the most important magnetic material in industrial applications. The general applications include volt relays or pulse transformers from the generator, automotive, and transformer sectors.
|
Applications |
Oriented silicon steel |
Non-oriented silicon steel |
Applications |
Oriented silicon steel |
||||||
|
HiB steels |
General oriented silicon steel |
Thin oriented silicon steel |
High grade non-oriented silicon steel |
Middle grade non-oriented silicon steel |
Low grade non-oriented silicon steel |
HiB steel |
General oriented silicon steels |
Thin oriented silicon steel |
||
|
Thickness (mm) |
Thickness (mm) |
|||||||||
|
0.23,0.27,0.30 |
0.27,0.30,0.35 |
0.15, 0.20 |
0.35,0.50,0.65 |
0.35, 0.50 |
0.50, 0.65 |
0.23,0.27,0.30 |
0.27,0.30,0.35 |
0.15, 0.20 |
||
|
Large Motors |
★ |
★ |
|
★ |
★ |
|
Large Motors |
★ |
★ |
|
|
Medium-sized motor |
|
|
|
★ |
★ |
|
Medium-sized motor |
|
|
|
|
Small motor |
|
|
|
|
★ |
|
Small motor |
|
|
|
|
Micro motor |
|
|
|
|
★ |
|
Micro motor |
|
|
|
|
Sealing motor |
|
|
|
★ |
★ |
|
Sealing motor |
|
|
|
|
Intermittent motor |
|
|
|
|
★ |
|
Intermittent motor |
|
|
|
|
IF motor |
|
|
|
★ |
|
|
IF motor |
|
|
|
|
Compressor |
|
|
|
|
|
|
Compressor |
|
|
|
|
Rectifier |
|
|
|
★ |
★ |
★ |
Rectifier |
|
|
|
|
Choke |
|
|
|
|
★ |
★ |
Choke |
|
|
|
|
Relay |
|
|
|
★ |
★ |
|
Relay |
|
|
|
|
Electromagnetic switch |
|
|
|
★ |
★ |
|
Electromagnetic switch |
|
|
|
|
Large power transformer |
★ |
★ |
|
|
|
|
Large power transformer |
★ |
★ |
|
|
Small & medium power transformer |
★ |
★ |
|
★ |
|
|
Small & medium power transformer |
★ |
★ |
|
|
Distribution transformer |
★ |
★ |
|
|
|
|
Distribution transformer |
★ |
★ |
|
|
Regulator |
★ |
★ |
|
★ |
|
|
Regulator |
★ |
★ |
|
Cold Rolled Oriented Silicon Steel Coil Packaging

Hot Tags: m15 m19 silicon steel coil, China m15 m19 silicon steel coil suppliers, CRNGO Electrical Steel Coil
Previous
M15 Silicon Steel CoilYou Might Also Like
Send Inquiry