What Is The Hardness Of Inconel 600?

What is the hardness of Inconel 600?

 

 

 

Nickel Alloy 600 Products supplier in China
Inconel is a versatile alloy, which is used in several industries. The Inconel 600 is a nickel-chromium alloy, which is highly resistant to corrosion. This alloy doesn't dissociate or deform easily under high pressures or elevated temperatures. Made up of superior strength the Inconel Alloy 600 has excellent mechanical properties. It has a minimum tensile strength of 760Mpa and a minimum yield strength of 585Mpa. These alloys can be easily elongated by 10% and still possess excellent workability. We are the leading Inconel 600 suppliers in the country. We supply high-quality products through all our outlets.

Check Inconel Alloy 600 Material Price per kg in China
The Inconel 600 melting point is in the range between 1354 to 1413 degrees C. This enables them to be used in heat treatment systems, chemical, food processing, phenol condensers, pressure vessels, etc. In the Inconel 600 thermal, conductivity is between 70 to 800 degrees F. They have this conductivity between 14.8 W/m·K to 20.9 W/m·K metric units. This helps in reducing running costs and operating material. The Inconel 600 machinability enables it to be drawn in square, rectangular, circular, and various other shapes. This alloy shows resistance against post-weld carburization and graining. The products of this grade are available in threaded, plain, and beveled ends. There are a few Inconel Alloy 600 equivalent grades. One of them is the UNS No6600 grade, which has similar strengths and mechanical properties as the 600 Inconel grade. These products are hardened as they are annealed after the hot-rolling process. Under the guidance of our workers, all our products are manufactured using the best raw materials and latest technology.

What is the hardness of Inconel 600?What is the hardness of Inconel 600?

Inconel 600 Specification

View Inconel 600 Equivalent, Melting Point, Thermal Conductivity, Composition, Machinability and Hardness

Standards Inconel 600
UNS N06600
Werkstoff Nr. 2.4816

 

Inconel Alloy 600 Chemical Compostion

  Inconel 600
Ni 72.0 min
Cr 14.0 – 17.0
Fe 6.0 – 10.0
C 0.15 max
Mn 1.0 max
S 0.015 max
Si 0.5 max
Cu 0.5 max

Inconel Alloy 600 Mechanical Strength

Density 8.47 g/cm3
Melting Point 1413 °C (2580 °F)
Tensile Strength Psi – 95,000 , MPa – 655
Yield Strength (0.2%Offset) Psi – 45,000 , MPa – 310
Elongation 40 %

 

Inconel 600 Application

Inconel 600 uses in Thermocouples

Inconel 600 uses in Nuclear Components

Inconel 600 uses in Paper & Pulp Industry

Inconel 600 uses in Heat Exchanger

Inconel 600 uses in Chlorination Equipment

Inconel 600 uses in Petrochemical