Mar 13, 2025 Leave a message

What Is The Grade Inconel 718?

What is the grade Inconel 718?

 

 

Inconel 718 is a Gamma Prime hardened alloy with excellent mechanical properties at both high and low temperatures. Suitable for temperatures up to about 1300 F. Easily machined and age hardened.

Excellent strength from -423°F to 1300°F (-253°C to 705°C). Age hardenable, weldable in the fully aged condition, excellent oxidation resistance up to 1800°F (980°C). Typically sold in the solution annealed condition, but can be ordered aged, cold worked, or cold worked and aged.

What is the grade Inconel 718?What is the grade Inconel 718?

Applications
Inconel 718 uses tend to be in the areas of gas turbine components and cryogenic tanks. Jet engines, pump bodies and parts, rocket engines and thrust reversers, nuclear fuel element gaskets, hot extrusion tools. Other common uses are high strength bolts and downhole shafting.

Chemistry

Chemical Requirements

 

Ni

Fe

Mo

Mn

Si

Cr

C

Max

55.0

Bal

3.30

0.35

0.35

21.0

0.08

Min

50.0

 

2.80

   

17.0

 

 

Mechanical Property Requirements

 

Ultimate Tensile

Yield Strength (0.2% OS)

Elong. in 2 in. (50mm) or 4D min, %

R/A

Hardness Brinell

Min

185 KSi

150 KSi

12

15

331

Max

         

Min

1275 MPa

1034 MPa

     

Max

         