Recently, GNEE has successfully delivered 160 tons of high-quality Inconel718 round bars to Japanese customers.
In order to ensure the smooth progress of this delivery, our team has made great efforts in every link such as production, quality control, packaging and logistics.
We strictly produce in accordance with international standards and customer requirements to ensure that each round bar meets the chemical composition and mechanical property standards of InConel718. At the same time, we also conduct comprehensive quality inspections on the round bars to ensure that their quality reaches the highest level.
InConel718 bar specifications:
InConel718 black round bar: Φ50-600, L1000-4000 30 tons
InConel718 polished round bar: Φ60-600, L1000-5000 45 tons
InConel718 hot-rolled round bar: Φ20-50, L1000-5000 15 tons
InConel718/ cold-drawn round bar: Φ4-20, L1000-5000 16 tons