There are wide stainless tubing dimensions to choose from, large diameter, heavy wall, or small diameter is available, the schedule number refers to the wall thickness of the stainless steel pipe, there are several Schedule numbers to meet different requirements, including SCH.5S, SCH.10, SCH.10S, SCH.20, SCH.30, SCH.40, SCH40S, SCH.80, SCH80S and larger Schedule No., when the number increases, the thicker the wall thickness with the same NPS dimensions, also the wall thickness changes based on the nominal pipe size (NPS).
Stainless Steel Pipe Specifications
| Specifications | ASTM A312, A358, A376, A409, A778 |
|---|---|
| Grade | 304/304L, 316/316L |
| Pipe Manufacture | Wlded Or Seamless |
| Finish | Annealing, Bright Annealing, Polishing |
| NPS | 1/8″ – 24″ |
| Schedule | Sch5 – Sch160 |
| Ends | Plain Ends, Beveled Ends |
Stainless Steel Pipe Dimensions, Wall Thickness And Weights
| Nominal Pipe Size (Inches) |
Outside Diameter |
Schedule | ||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| 5S | 10S | 40S | 80S | |||||||
| (Mm) | (Inches) | Wall Thickness And Weight | ||||||||
| Mm (In) |
Kg/M | Mm (In) |
Kg/M | Mm (In) |
Kg/M | Mm (In) |
Kg/M | |||
| 1/8 | 10.3 | 0.405 | – | – | 1.25 (0.049) |
0.28 | 1.73 (0.068) |
0.37 | 2.42 (0.095) |
0.47 |
| 1/4 | 13.7 | 0.540 | – | – | 1.66 (0.065) |
0.49 | 2.24 (0.088) |
0.63 | 3.03 (0.119) |
0.80 |
| 3/8 | 17.2 | 0.675 | – | – | 1.66 (0.065) |
0.63 | 2.32 (0.091) |
0.85 | 3.20 (0.126) |
1.10 |
| 1/2 | 21.3 | 0.840 | 1.65 (0.065) |
0.81 | 2.11 (0.083) |
1.00 | 2.77 (0.109) |
1.27 | 3.74 (0.147) |
1.62 |
| 3/4 | 26.7 | 1.050 | 1.65 (0.065) |
1.02 | 2.11 (0.083) |
1.28 | 2.87 (0.113) |
1.68 | 3.92 (0.154) |
2.20 |
| 1 | 33.4 | 1.315 | 1.65 (0.065) |
1.30 | 2.77 (0.109) |
2.09 | 3.38 (0.133) |
2.50 | 4.55 (0.179) |
3.24 |
| 1 1/4 | 42.2 | 1.660 | 1.65 (0.065) |
1.66 | 2.77 (0.109) |
2.69 | 3.56 (0.140) |
3.39 | 4.86 (0.191) |
4.47 |
| 1 1/2 | 48.3 | 1.900 | 1.65 (0.065) |
1.91 | 2.77 (0.109) |
3.11 | 3.69 (0.145) |
4.06 | 5.08 (0.200) |
5.41 |
| 2 | 60.3 | 2.375 | 1.65 (0.065) |
2.40 | 2.77 (0.109) |
3.93 | 3.92 (0.154) |
5.45 | 5.54 (0.218) |
7.49 |
| 2 1/2 | 73.0 | 2.875 | 2.11 (0.083) |
3.69 | 3.05 (0.120) |
5.26 | 5.16 (0.203) |
8.64 | 7.01 (0.276) |
11.4 |
| 3 | 88.9 | 3.500 | 2.11 (0.083) |
4.52 | 3.05 (0.120) |
6.46 | 5.49 (0.216) |
11.3 | 7.62 (0.300) |
15.3 |
| 3 1/2 | 101.6 | 4.000 | 2.11 (0.083) |
5.18 | 3.05 (0.120) |
7.41 | 5.74 (0.226) |
13.6 | 8.08 (0.318) |
18.6 |
| 4 | 114.3 | 4.500 | 2.11 (0.083) |
5.84 | 3.05 (0.120) |
8.37 | 6.02 (0.237) |
16.1 | 8.56 (0.337) |
22.3 |
| 5 | 141.3 | 5.563 | 2.77 (0.109) |
9.46 | 3.41 (0.134) |
11.6 | 6.56 (0.258) |
21.8 | 9.53 (0.375) |
31.0 |
| 6 | 168.3 | 6.625 | 2.77 (0.109) |
11.3 | 3.41 (0.134) |
13.9 | 7.12 (0.280) |
28.3 | 10.98 (0.432) |
42.6 |
| 8 | 219.1 | 8.625 | 2.77 (0.109) |
14.8 | 3.76 (0.148) |
20.0 | 8.18 (0.322) |
42.5 | 12.70 (0.500) |
64.6 |
| 10 | 273.1 | 10.750 | 3.41 (0.134) |
22.7 | 4.20 (0.165) |
27.8 | 9.28 (0.365) |
60.4 | 12.70 (0.500) |
81.5 |
| 12 | 323.9 | 12.750 | 3.97 (0.156) |
31.3 | 4.58 (0.180) |
36.1 | 9.53 (0.375) |
73.9 | 12.70 (0.500) |
97.4 |
Stainless Steel Grade
Stainless steel materials have excellent properties to use in high pressure, high temperature and corrosion environments, besides below stainless steel grades, we also offer other alloy steel on request.
| 300 Series | 400 Series | Others |
|
301, 302, 303 304, 304L, 304H 316, 316L, 316H, 316Ti 317, 317L, 317LN 321, 321H 347, 347H 310S |
409, 409L 430 439 441 443 436L 444 |
904L S31803 S32205, 2205 S32750, 2507 254SMO |
GNEE STEEL offer Schedule 40/40S wall thickness ss pipe to meet various applications, the commonly used grades have 304/304L 316/316L stainless steel, these grades possess excellent corrosion resistance suited to many industries, such as oil & gas, petrochemical engineering & chemical industry.