Inconel Alloy Uns N06600 Plate
Gnee Steel
Learn about Inconel Alloy Uns N06600 Plate Information
Inconel alloy UNS N06600, commonly known as Inconel 600, is a nickel-chromium alloy prized for its excellent corrosion resistance, high strength, and high-temperature performance. It is commonly used in plate form in a variety of applications, including chemical processing, food processing, and nuclear reactors.

Gnee Steel
What are the specifications for Alloy 600?
Alloy 600 is a nickel-chromium alloy designed for use in temperatures ranging from cryogenic to 2000°F (1093°C). The alloy's high nickel content makes it quite resistant to reducing conditions and corrosion from a wide range of organic and inorganic compounds.

Inconel 600 Sheet, Plate & Plate Specifications |
||
| Specifications | ASTM / ASME SB 168 | |
| Size | 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm | |
| Thickness | 0.1mm to 12 mm Thk | |
| Form | Sheets, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange) | |
| Finish | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) | |
| Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. | |
Inconel 600 Plate, Sheet & Plate Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| Inconel 600 | 0.15 max | 1.00 max | 0.50 max | 0.015max | 0.50 max | 6.00 – 10.00 | 72.00 min | 14.00 – 17.00 |
Alloy 600 Sheets, Plates & Sheets Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 600 | 8.47 g/cm3 | 1413 °C (2580 °F) | Psi – 95,000 , MPa – 655 | Psi – 45,000 , MPa – 310 | 40 % |
Inconel 600 Plate, Plate, and Sheet Applications
Offshore Oil Drilling Companies
Power Generation
Petrochemicals
Natural Gas Processing
Specialty Chemicals
Pharmaceuticals
Pharmaceutical Equipment
Chemical Equipment
Seawater Equipment
Heat Exchangers
Condensers
Pulp and Paper

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.