Incoloy 800 pipe is a nickel-iron-chromium alloy known for its excellent resistance to high temperatures, oxidation, carburization, and chloride stress corrosion cracking. It is widely used in a variety of industrial fields, including petrochemical processing, power generation, and heat treatment equipment.

What is Incoloy 800 Pipe?

Incoloy 800 Pipe is a nickel-iron-chromium alloy pipe that has good strength and excellent resistance to oxidation and carburization in high temperature environments. It has excellent corrosion and heat resistance, making it an ideal choice for applications such as petroleum refining, chemical processing, and power generation.
Characteristics of Incoloy 800 Tube
Incoloy 800 Tube is a nickel-iron-chromium alloy with excellent resistance to oxidation, sulfidation and carburization. It has high strength and good corrosion resistance in both high and low temperature environments. The alloy can also be used in severe applications such as acid chlorides and alkaline salt solutions, and is ideal for heat exchangers, condensers, evaporators, combustion chambers, sleeves, etc. Its advantages include: excellent hot workability after annealing; excellent stress rupture properties; excellent creep rupture strength; can withstand temperatures up to 1260°C (2300°F); does not embrittle after welding or thermal shock; excellent room temperature formability and very good weldability.
Applications of Incoloy 800 Tube
Incoloy 800 Tube is a nickel-iron-chromium alloy that offers excellent resistance to high temperature corrosion. It has excellent thermal stability and maintains its strength even when exposed to high temperatures for extended periods of time. Its main applications include heat exchangers, condensers, storage tanks, and piping systems in refineries, nuclear power plants, chemical plants, industrial furnaces, etc. Its excellent creep and stress rupture properties make it an ideal choice for high temperature components operating under pressure, such as valves or structural components. It is also widely adopted for its excellent resistance to sulfur compounds at high temperatures, making it an essential material for pipeline networks that transport sour liquids or gases. In addition, with continuous use at temperatures of 1200°F (649°C), it offers significant advantages over austenitic steels when used in welded structures with similar grain size control requirements.
Advantages of using Incoloy 800 Tubes
Incoloy 800 tubes have many unique advantages that make them ideal for a wide range of industries. These advantages include excellent resistance to water and high temperature corrosion, good formability and weldability, and excellent strength and toughness even at high temperatures. They are also resistant to oxidation, carburization, nitridation, and sulfidation. Incoloy 800 tubes exhibit excellent creep rupture performance up to 1500°F (816°C). This makes them ideal for high temperature furnace components, heat exchangers, and other parts.

Gnee Steel is a supplier of Incoloy 800 Pipe, covering pipes: Seamless pipes: Size: 4 - 219 mm; Thickness: 0.5 - 20 mm; Welded pipes: Size: 5.0 - 1219.2 mm; Thickness: 0.5 - 20 mm, Plates: Plate thickness 0.1 to 100 mm; Plate width 10-2500 mm, Strips, Alloy round bar sizes: diameter 3-800 mm;, Flat bar sizes: thickness 2-100 mm; Width: 10-500 mm, Hexagonal bar sizes: 2-100 mm;, Wire and extruded profiles. We work with steel mills to provide customers with 625 alloy, and its products meet or exceed many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Incoloy 800 Pipe, Tube, Pipe, Plate, Strip, Plate, Round Bar, Flat Bar, Forged Billet, Hexagon, Wire and Extruded Profiles. Feel free to contact us for a quote at ss@gneesteel.com