Stainless steel grade 317L is a low carbon version of grade 317 stainless steel. It has the same high strength and corrosion resistance as 317 steel but can produce stronger welds due to the low carbon content
ASTM A312 TP317L (UNS S31703) is a molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless steels such as Alloy 304. In addition, Alloy 317L offers higher creep, stress-to-rupture, and tensile strength at elevated temperatures than conventional stainless steels. It is a low carbon or "L" grade which provides resistance to sensitization during welding and other thermal processes.


ASTM A312 TP317L Stainless steel Pipes,UNS S31703 1.4438 Seamless pipe
Chemical Composition Of ASTM A312 TP 317L SS Seamless Pipe
| SS | 317 | 317L |
| Ni | 11–14 | 11–15 |
| N | – | – |
| Cr | 18 – 20 | 18 – 20 |
| C | 0.08 max | 0.035 max |
| Si | 1 max | 1 max |
| Mn | 2 max | 2 max |
| P | 0.040 max | 0.040 max |
| S | 0.030 max | 0.03 max |
| Mo | 3.00 – 4.00 | 3 – 4 |
| Mechanical Properties of Astm A213 TP 317L | |
| Density | 8.0 g/cm3 |
| Melting Point | 1454 °C (2650 °F) |
| Tensile Strength | Psi – 75000, MPa – 515 |
| Yield Strength (0.2%Offset) | Psi – 30000, MPa – 205 |
| Elongation | 35% |
How to order our ASTM A312. TP317L Seamless pipes?
Stainless Steel Seamless Pipe size DN100 (OD114.3MM) x S.80S/SX (8.56mm) x 6000mm. ASME B36.19M, Material: ASTM A312. GR. TP317L. N.W: 133.92KG/PC.Contact US :ss@gneesteel.com