Alloy 600
Incoloy 600 can withstand the high temperature of 1093 ℃, which is a good engineering material with good hot workability, corrosion resistance, oxidation resistance and plasticity.
Characteristic:
1. It has good corrosion resistance, specifically, it can resist the corrosion of various corrosive media, such as waste gas, alkaline solution, etc.
2. Good mechanical properties.
3. Good welding performance.


Chemical compositon:
|
C |
Mn |
Ni |
Si |
P |
S |
Cr |
Fe |
Al |
Ti |
Cu |
|
0.015 |
≤1.00 |
≥72 |
≤0.5 |
≤0.015 |
≤0.015 |
14.0~17.0 |
6.0~10.0 |
≤0.3 |
≤0.3 |
≤0.5 |
Physical property:
|
density |
melting point |
magnetic |
|
8.43g/cm3 |
1354-1413℃ |
/ |
Field of Application:
Heat treatment furnaces.
Production environment of corrosive alkali metals.
Various high-precision components.
Chemical food, nuclear reactor and petrochemical industry.