Monel ASTM B164 UNS N04400 polished Round Bars
Specification: ASTM B 164
Dimensions: ASTM, ASME
Dimensions: Diameter: 3-~800mm
Length: 100 mm to 3000 mm and above
Shape: Round, Square, Hexagonal (A/F), Rectangular, Flat
Type: ASTM B 164 Monel 400 Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel astm b164 uns n04400 polished round bars in China. If you're going to wholesale high quality monel astm b164 uns n04400 polished round bars made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel ASTM B164 UNS N04400 polished Bars introduce
Monel UNS N04400 polished Round Bars


Gnee Steel is one of the leading manufacturers of Monel 400 Round Bars, Rods, and its raw materials are of high quality, ensuring the highest quality of industry standard products. Monel 400 Round Bars are a rock-hard solution alloy that can be easily toughened by cold working. Moreover, Monel 400 Rods also possess properties like good weldability, high strength, and good corrosion resistance.
Monel 400 Round Bars and Rods manufactured by Gnee Steel are not only known for their high quality and strength. These Monel 400 Round Bars, Rods also known as UNS N04400, can be further customized in size and thickness as per the specific needs of our valued clients. We offer these Round Bars and Rods at industry leading costs.
The ASTM B164 specification refers to nickel copper alloys in the form or hot or cold worked products. The ASTM B164 UNS N04400 round bars are widely used in marine and thermal applications. GNEE Steel apart from offering great quality ASME SB164 rounds at affordable prices, our customer-friendly team is always there to assist you. Contact us today to get custom-made round bars delivered to your doorstep on time.
| Specifications | ASTM B164, AMS 4675, AMS 4730, AMS 4731 |
|---|---|
| Grade | Monel 400 – UNS N04400, Nickel Alloy 400 (66 Ni/34 Cu) |
| Technique | 400 Monel Cold Drawn, Hot Rolled, Forged Round Bar, Rod, Cold Rolled |
| Tolerance | H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients' requirements |
| Finish | Cold (bright) drawn, centreless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centreless Ground & Black |
| Round bar size | Diameter: 3-~800mm |
| Hex Bar size | 2-100mm A/F |
| Flat bar size | Thickness: 2 -100mm |
| Width: 10 to 500mm | |
| Square bar size | 4 to 100mm |
| Section | 3.0 to 12.0mm thickness |
| Form | Precision Ground Bar, Flat Bar, Square, Round, Half Round Bar, Rod, Rectangle, Hex (A/F), T-Bar, Channel Bar,Blocks, Round Rod, Threaded, Profiles, Billet, Ingot, I/H Bar, Forging, Rings, Hollow, Triangle etc. |
| Rectangles Size | 33 x 30mm to 295 x 1066mm |
| Surface | Cold Drawn, Bright, Sand Blasting Finished, Hot Rolled Pickled, Hairline, Polished |
| Processing | Bar cutting to 650mm |
| Billet Size | 1/2″ to 495mm Diameter |
| Channel Bar | 80 x 40mm to 150 x 75mm section; 5.0 to 6.0mm thickness |
| Hollow Bar | 32mm OD x 16mm ID to 250mm OD x 200mm ID) |
| Angle bar size | 3mm*20mm*20mm~12mm*100mm*100mm |
| Condition | Hardened & tempered, annealed |
| Our 400 Monel Round bar conforms to NACE MR0175/ISO 15156 | |
Monel ASTM B164 UNS N04400 Round Bars

The Condition Of ASME SB 164 UNS N04400 Rod
The common conditions of ASME SB 164 UNS N04400 rods will include annealing. Herein, the material is heated to a specific temperature and then cooled to relieve stress. The process helps improve the machinability and formability of alloy 400.
They can also be cold worked to achieve specific mechanical properties.
UNS N04400 rods can age hardened to improve their strength and hardness.
Some bars can also be supplied in as-drawn condition without undergoing any additional heat treatment.
Difference Between Hot-Worked And Cold-Worked N04400 Bar
The hot worked ASME SB164 N04400 rectangular bars are shaped at elevated temperatures above its recrystallization temp. After the metal is heated, it will get easier to deform and shape. The cold worked bars are shaped at room temperature without significant heating.
Hot working decreases the hardness and improves the ductility of the bars. Cold working enhances the hardness and strength compared to the hot worked bars.
Hot worked bars give an oxidized surface whereas ASTM B164 cold drawn bars have a smooth & clean finish.
Cold worked UNS N04400 bright bars have a tighter dimensional tolerance than the hot worked ones.
GNEE Group Product Packaging
Monel 400 Round Bars


FAQ
Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.
Hot Tags: Monel ASTM B164 UNS N04400 polished Round Bars, China Monel ASTM B164 UNS N04400 polished Round Bars suppliers, monel alloy, soldering alloy, alloy consultation, alloy disadvantage, alloy rolling, alloy wholesaler
Previous
Monel R405 Alloy PipeYou Might Also Like
Send Inquiry