Monel 400 Plate
video

Monel 400 Plate

Alloy Name: Monel 400
UNS: N04400, W.Nr.2.4360
Forms: Plate, sheet, strip, seamless/welded pipe‑tube, bar, forging, fitting, flange
Matrix type: Solid‑solution nickel‑copper alloy, hardenable only by cold‑work
Key features: Excellent seawater & hydrofluoric acid resistance, good low‑temp toughness
Applicable standards: ASTM B127, B164, B165, B725, B730, B366
Delivery condition: Annealed / cold‑drawn & stress‑relieved
Mandatory inspection: PMI, UT / MT, dimensional verification
Typical industries: Marine, desalination, chemical‑HF equipment, heat‑exchanger, oil‑gas
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel 400 plate in China. If you're going to wholesale high quality monel 400 plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel 400 Plate description

 

Gnee Steel is a well-known Chinese exporter and supplier of Monel 400 alloy plates, sheets, and coils, offering a wide variety of specifications and designs. Our professional team conducts rigorous inspections of these products to ensure they meet the highest quality standards. Monel 400 coils and Monel 400 gaskets are common forms of this alloy and are widely used in various manufacturing sectors.

 

Monel 400 Sheet & Plates

GNEE Monel 400 Plate

 

Monel 400 alloy plates are among the most durable and versatile materials in the industry. They are commonly used in applications requiring corrosion resistance, low gas and oil permeability, and high strength. Monel 400 alloy plates come in various types, including hot-rolled and cold-rolled Monel 400 plates. Hot-rolled plates are manufactured using a high-temperature, high-pressure process, while cold-rolled plates are processed at lower temperatures to increase their hardness. Other types of Monel 400 alloy plates include perforated plates, embossed plates, and decorative plates.

 

Monel 400 alloy plates are widely used across various industries, including marine, chemical, oil and gas, and aerospace. They are ideal for applications requiring high corrosion resistance and high strength, such as heat exchangers, evaporator tubes, storage tanks, pump shafts, marine components, valves, and fittings. Monel 400 alloy plates are also used in seawater environments, which are typically rich in chlorides and acidic.

 

At Gnee Steel, we offer high-quality monel 400 Plate in various sizes and thicknesses, and provide custom cutting, surface treatment, and global delivery services to meet your specific project needs.

Contact now

Monel 400 Sheet
Monel 400 Plates
Monel 400 Coils

 

Monel 400 Plate Specification

 

Specifications ASTM B127 / ASME SB127
Dimension Standard MSRR, AMS, BS, JIS, AISI, ASTM, GB, DIN, EN, etc
Size Range Cold Rolled : 0.5-6.4 mm
Hot Rolled : 3.0–10.0 mm
Width 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc
Length 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc
Thickness 0.3 mm to 120 mm
Hardness Half Hard, Soft, Hard, Quarter Hard, Spring Hard
Finish 2B, 2D, BA NO (8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc.
Form Sheet, Plate, Strip, Flats, Clad Plate, Coils, Foils, Plain Sheet, Flat Shim, Flat Sheet, Shim Sheet, Rolling Sheet, Rolling Plate, Rolls, Blank (Circle), soft annealed, descaled, tread plate, sheared, annealed
Value Added Service Cladding, Heat Treatment, Annealed, Pickling, Polish, Rolling, Cutting, Bending, Forging, Minor Fabrication Etc.
Profiling Plasma Plate Cutting
Laser Plate Cutting
Oxy-propane Flame Cutting

 

Monel 400 Plate Specification

 

Monel 400 Sheets Equivalent Grade

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Monel 400 2.4360 N04400 NW 4400 NA 13 МНЖМц 28-2,5-1,5 NU-30M NiCu30Fe

 

400 Monel Alloy Sheets Chemical Composition

Grade C Mn Si Cu S Ti Ni Al Fe
Monel 400 0.3 max 2.0 max 0.5 max 28.0 – 34.0 0.02 max - 63.0 min 0.50 max 1.0 – 2.5

 

Monel Alloy 400 Plate Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Monel 400 8.8 g/cm3 1350 °C (2460 °F) Psi – 80000 , MPa – 550 Psi – 35000 , MPa – 240 40 %

 

Monel Alloy 400 Sheet Manufacturing Process

 

Monel Alloy 400 Sheet Manufacturing Process

Monel Alloy 400 Sheet Manufacturing Process

 

Monel 400 Plate Technical Data Sheet

 

Monel 400 Sheet Size Chart

Size (in inches)

Size (in mm)

.125"

3.18mm

.134"

3.40mm

.156"

3.96mm

.187"

4.75mm

.250"

6.35mm

.312"

7.92mm

.375"

9.53mm

.500"

12.7mm

.600"

15.9mm

.750"

19.1mm

.875"

22.2mm

1"

25.4mm

1.125"

28.6mm

1.250"

31.8mm

1.500"

38.1mm

1.750"

44.5mm

2"

50.8mm

2.500"

63.5mm

3"

76.2mm

 

Dimension standards of Monel 400 Grade Cold Rolled Plate

Plate Surface finish Gauge (in) Width (max in)
2B – Cold rolled, heat treated, pickled, skin passed Plate 10–24 72*
2D – Cold rolled, heat treated, pickled plate 12–24 60
BA Mexinox only 18–28 48
Polished plate (not brushed) 11–24 60
Temper rolled plate Mexinox only 13–29 48

 

Plate Surface finish Thickness (mm) Width (max mm)
2B – Cold rolled, heat treated, pickled, skin passed plate 0.25–8.0 2032
2D – Cold rolled, heat treated, pickled plate 0.4–6.35 1524
2E – Cold rolled, heat treated, mechanically descaled plate 0.4–8.0 2032
2R – Cold rolled, bright annealed plate 0.25–3.5 1524
2H – Work hardened plate 0.4–6.35 1524
Polished, brushed plate 0.5–4.0 1524

 

The delivery time for Monel 400 Plate varies depending on the location

 

Cost Changes 5 % extra
Export to Delivery Time
UAE 5 days
Qatar 7
France 30
Kuwait 10
USA 40-60
Saudi Arabia 7
Oman 5
Italy 30
Uk 30

 

Monel 400 Plate are in stock and available for immediate shipment to meet urgent needs

 

DIN 17750 Perforated Sheet

DIN 17750 Perforated Sheet

Monel Alloy 400 Checker Plate

Monel Alloy 400 Checker Plate

Alloy Monel 400 Shim Stock

Alloy Monel 400 Shim Stock

Alloy UNS N04400 0.5mm thick x 1000mmx1000mm

Alloy UNS N04400 0.5mm thick x 1000mmx1000mm

400 Alloy 0.5mm thick x 1000mmx2000mm Plate

400 Alloy 0.5mm thick x 1000mmx2000mm Plate

Alloy Monel 400 Strip Tape

Alloy Monel 400 Strip Tape

2.4360 Monel 400 Hot Rolled Plate

2.4360 Monel 400 Hot Rolled Plate

ASTM B127 Alloy 400 Strip

ASTM B127 Alloy 400 Strip

Alloy Monel 400 Coil

Alloy Monel 400 Coil

 

Products and services offered by Gnee Steel

 

Applications of Monel 400 Plate

 

Aerospace: Jet engine components, gas turbine parts, rocket engines, and fasteners.

Oil and Gas: Downhole drill pipes, wellhead components, valves, and pump assemblies.

Chemical Industry: High-temperature reactors and pipelines.

Marine: Submarine components and high-strength shafts.

Nuclear Energy: Reactor core and control rod components.

Monel 400 Plate

Packaging method for Alloy 718 Pipe Fitting

Packaging method for Alloy 400 Plate

 

Gnee Steel uses the safest and most effective packaging methods for all types of cargo transportation. Our packaging methods include:

Wooden crates
Wooden pallets
Shrink wrap packaging
Cardboard boxes
Wooden crates (slatted)

 

Monel 400 Plate Price List

 

Price List of Monel 400 Plate Monel 400 Sheet Price in India (INR) Monel 400 Sheet Price in USD Monel 400 Sheets Price in UAE (Dirham)
Monel 400 Sheet Price In Mumbai ₹ 1166 $ 14.24 USD 52.28 AED
Monel 400 Sheet Price List ₹ 1300 $ 15.87 USD 58.29 AED
Monel Alloy 400 Sheet Price ₹ 500 $ 6.11 USD 22.43 AED
Price of Alloy 400 Plates ₹ 645 $ 7.87 USD 28.92 AED
Monel Alloy 400 Plate Price Today ₹ 480 $ 5.86 USD 21.52 AED
Nickel Alloy 400 Plate Price List ₹ 356 $ 4.35 USD 15.96 AED
Monel 400 Plate Price List ₹ 1205 $ 14.71 USD 54.03 AED

 

About Gnee Steel

 

Gnee Steel

 

About Gnee Steel

Request the latest Monel 400 Plate price list. Please call +8615824687445 or email ss@gneesteel.com for information on available stock and the latest price list for Nickel 400 Plate.

modular-1
Please contact us to get a quick quote for the Monel 400 Plate you need

We supply these Monel 400 Sheet and tubes according to DIN, ISO, JIS, or ANSI/ASME standards.

FAQ

Q: Can Monel 400 alloy plates be welded?

A: Yes, Monel 400 alloy plates can be welded using standard welding methods such as TIG welding, MIG welding, and arc welding. To maintain corrosion resistance and mechanical properties, it is recommended to use Monel 400 or a similar nickel-copper alloy filler metal.

Q: What is the thickness range of Monel 400 alloy plates?

A: The thickness of Monel 400 alloy plates typically ranges from 0.3 mm to 20 mm, but customized thicknesses can also be provided to meet industrial requirements.

Q: What factors affect the price of Monel 400 alloy plates?

A: The price of Monel 400 alloy plates is influenced by several factors, including the size and thickness of the plates, the quantity ordered, surface finish, and any custom or processing requirements. Market prices for nickel and copper alloys, as well as transportation and handling costs, also affect the final price.

Hot Tags: monel 400 plate, China monel 400 plate suppliers, alloy raw material, alloy reputation, surface finish alloy, Monel 500, machining tolerance alloy, alloy development

Send Inquiry

whatsapp

Phone

E-mail

Inquiry