Product name: Hastelloy/C-276/UNS N10276

International common names: Hastelloy, C-276, INCONEL Alloy C-276, HC-276, Hastelloy C-276, UNS N10276, W.-Nr. 2.4819, ATI C-276, Nicrofer 5716 hMoW-Alloy C-276, NAS NW276
Implementation standards: ASTM B575/ASME SB-575, ASTM B574/ASME SB-574, ASTM B622/ASME SB-622, ASTM B619/ASME SB-619, ASTM B366/ASME SB-366, ASTM B564/ASME SB-564

Main ingredients:

Carbon (C) ≤ 0.01, Manganese (Mn) ≤ 1.00, Nickel (Ni) ≥ 57, Silicon (Si) ≤ 0.08 Phosphorus (P) ≤ 0.04, Sulfur (S) ≤ 0.03, Chromium (Cr) 14.5~16.5, Iron (Fe)4.0~7.0, molybdenum (Mo)15.0~17.0, tungsten (W)3.0~4.5, cobalt (Co) ≤2.5

Physical properties: C-276 density: 8.9g/cm3, melting point: 1325-1370 ℃, magnetic properties: none

Heat treatment: heat preservation between 1150-1175℃ for 1-2 hours, rapid air cooling or water cooling.

Mechanical properties: Tensile strength: σb≥690Mpa, Yield strength σb≥275Mpa: Elongation: δ≥40%, Hardness ≤100 (HRB)

Which standard does Hastelloy C276 plate comply with?

Which standard does Hastelloy C276 plate comply with?

Corrosion resistance and main use environment:

Hastelloy C-276 is a tungsten-containing nickel-chromium-molybdenum alloy with extremely low silicon-carbon content and is considered a universal corrosion-resistant alloy. This alloy has the following characteristics: ① It has excellent corrosion resistance to most corrosive media in both oxidizing and reducing atmosphere states. ②Excellent resistance to pitting corrosion, crevice corrosion and stress corrosion. The higher molybdenum and chromium content makes the alloy resistant to chloride ion corrosion, and the tungsten element further improves the corrosion resistance. At the same time, C-276 alloy is one of the only materials resistant to corrosion by moist chlorine, hypochlorite and chlorine dioxide solutions, and has significant resistance to high-concentration chloride solutions such as ferric chloride and copper chloride. Corrosion resistance. It is suitable for sulfuric acid solutions of various concentrations and is one of the few materials that can be used in hot concentrated sulfuric acid solutions.
Supporting welding materials and welding processes: Hastelloy C-276 welding materials use ERNiCrMo-4 welding wire and ENiCrMo-4 welding rod. The welding material sizes are Φ1.0, 1.2, 2.4, 3.2, 4.0. The origin is: Hastelloy, United States, United States For SMC and Deutsche Nickel, please call us for welding procedures and instructions.

Inventory status: The stock sizes of C-276 alloy plates are 0.38mm-45mm, the stock sizes of bars are Φ12mm-Φ320mm, pipes, fittings and others can be customized according to customer requirements. The main origins of materials include Hastelloy Haynes in the United States, SMC in the United States, ATI in the United States, and Thyssenkrupp VDM in Germany. Provide original material certificate, customs declaration form and certificate of origin.

Application fields include: power plant desulfurization and denitrification environmental protection, petrochemical equipment, coal chemical industry, fluorine chemical industry, fine chemicals, PTA, aviation manufacturing, offshore platforms, seawater desalination, papermaking machinery, pharmaceutical equipment, heat exchange equipment, electrochemistry, metallurgy, nuclear energy, Chlor-alkali, shipbuilding, cement manufacturing, composite panels, acetic anhydride, salt production and plate heat exchangers, bellows expansion joints and other industries and products.

 