Corrosion resistance alloy 725 / UNS NO7725

Corrosion resistance alloy 725 / UNS NO7725

 

Inconel 725 has basically the same corrosion resistance as Inconel 625 and is widely used in various severely corrosive environments. Age-hardened Inconel 725 alloy is twice as strong as annealed Alloy 625. Because the strength of 725 alloy is developed through heat treatment rather than cold working, the ductility and toughness remain high. In addition, it can also provide strength to large or uneven parts that cannot be strengthened by cold working.

High nickel and chromium content provide corrosion resistance in reducing and oxidizing environments. The high molybdenum content enhances resistance to reducing media and provides a high degree of resistance to pitting and crevice corrosion. Additionally, the combination of elements makes the alloy resistant to hydrogen embrittlement and stress corrosion cracking.

The properties of Inconel 725 alloy lend themselves to a range of applications requiring excellent corrosion resistance and high strength. The alloy is used in hangers, landing joints, side bag mandrels and polished bore vessels in sour gas environments and is resistant to the effects of hydrogen sulfide, chloride and carbon dioxide. The alloy is also attractive for high-strength fasteners in marine applications because it resists corrosion, pitting and crevice erosion in seawater.

Corrosion resistance alloy 725 / UNS NO7725

Corrosion resistance alloy 725 / UNS NO7725

Common product names:

Inconel 725, Alloy 725, Nickel 725, UNS NO7725

Specification:

ASTM B805, NACE MR0715

Phase Characteristics of Inconel 725

The results show that the main strengthening mechanism of Inconel 725 alloy is the precipitation and fine grain strengthening of γ'/γ" phase. The strength of the alloy is mainly determined by the number and particle spacing of γ'/γ" phase. The smaller the spacing, the greater the intensity. The plasticity of the alloy is mainly determined by the amount of δ phase precipitation, which is not conducive to the improvement of plasticity. In addition, the amount of δ phase is also closely related to the grain size, and its pinning effect on the grains is not conducive to the growth of the grains. After 1.5 hours of solid solution at 996°C, the δ phase rarely precipitates in the form of particles at the grain boundaries. After 1 hour of solid solution at 1040°C, the δ phase is completely dissolved in the matrix. The precipitation of δ phase can be effectively reduced through appropriate heat treatment process.

Inconel 725 is resistant to pitting corrosion

Pitting corrosion of Inconel 725 and Inconel 718 alloys originates from precipitated MC carbides. Temperature has little effect on pitting corrosion of Inconel 725 alloy, and the critical pitting temperature is as high as 90±3°C. The hydrogen embrittlement resistance of Inconel 718 alloy is better than that of Inconel 725 alloy. The strength loss rates caused by hydrogen embrittlement are 27% and 31.6% respectively.

The optimal processing temperature of Inconel 725 alloy is 1100℃~1150℃, the strain rate is 0.1~1s-1, and the thermal deformation activation energy is 240.34 kJ/mol.

 