What material is UNS S32750 dual phase steel? 1.4410 corresponds to domestic brands

What material is UNS S32750 dual phase steel? 1.4410 corresponds to domestic brands

 

Chemical composition of 2507 duplex stainless steel:

C≤0.03, Si≤0.080, Mn≤1.2, Cr:24-26, Ni:6-8, S≤0.02, P≤0.035, Mo:3-5, N:0.24-0.32

After suitable solution treatment of 2507 stainless steel, the microstructure of this steel has an ideal dual-phase structure with an α/γ ratio of approximately 50/50. When the solid solution temperature is above 1050°C, the number of ferrite phases in steel will increase as the temperature increases, but due to the high nitrogen content, the proportion of steel phases will not change significantly below 1300°C. If this steel is not aged at different temperatures (or affected by heat), γ2 will be formed on the α+γ matrix and δ, χ, R, α` intermetallic phases and Cr2N and other oxides will precipitate. Due to the carbon content in the steel Low (generally 0.01%-0.02%), so there are generally no carbides in steel.

2507 Stainless Steel 2507 is a ferritic-austenitic (duplex) stainless steel, which combines the most beneficial properties of many ferritic steels and austenitic steels, due to the high chromium and molybdenum content of the steel. , so it has excellent resistance to pitting corrosion, crevice corrosion and uniform corrosion. The two-way microstructure ensures that the steel has high resistance to stress corrosion cracking and has high mechanical strength.

What material is UNS S32750 dual phase steel? 1.4410 corresponds to domestic brands

What material is UNS S32750 dual phase steel? 1.4410 corresponds to domestic brands

2507 stainless steel is used in the oil and gas industry; offshore Shipotian oil platforms (heat exchanger tubes, water treatment and water supply systems, fire protection systems, water spray systems, water stabilization systems; petrochemical equipment; desalination (desalination) equipment (and equipment) high-pressure pipes, seawater pipes); mechanical and structural components that require both high strength and high corrosion resistance; combustion (waste) gas purification equipment.

2507 duplex stainless steel national standards:

ASTM/ASME:A240-UNS S32750

EURONORM:1.4410 - X2 Cr Ni MoN 25.7.4

AFNOR:Z3 CN 25.06 Az

DIN/EN 1.4410, ASME SA-240

Corresponding to domestic brand 022Cr25Ni7Mo4N (S25073)

2507 duplex stainless steel corrosion resistance

1.General corrosion

The higher chromium and molybdenum content of SAF 2507 makes it highly resistant to overall corrosion against organic acids such as formic acid and acetic acid. SAF 2507 alloy is also highly resistant to inorganic acids, especially those containing chlorides. corrosion resistance.

Compared with 904L, SAF2507 has stronger corrosion resistance against dilute sulfuric acid mixed with chloride ions. 904L is an alloy in an austenitic state and is specifically designed to resist pure sulfuric acid corrosion.

Grade 316L cannot be used in hydrochloric acid environments, as it may be subject to local corrosion or overall corrosion. SAF2507 can be used in dilute hydrochloric acid environments and has strong resistance to spot damage and crevice corrosion.

2. Intergranular corrosion

The lower carbon content of nSAF 2507 greatly reduces the risk of carbide precipitation between the grains during heat treatment. Therefore, this alloy has a strong ability to resist carbide-related intergranular corrosion.

3. Stress corrosion cracking

The duplex structure of SAF 2507 makes it highly resistant to stress corrosion cracking. Due to its higher alloy content, SAF 2507 has better corrosion resistance and strength than 2205.

Cracks are almost inevitable in construction and other aspects, which makes stainless steel more susceptible to corrosion in chloride environments. SAF 2507 has a strong ability to resist crack corrosion. Isocorrosion curve of SAF 2507 in sulfuric acid containing 2000ppm chloride ions 0.1 mm/year; iso-corrosion curve in hydrochloric acid 0.1 mm/year.

Mechanical properties: SAF 2507 has high compressive strength, impact strength, low thermal expansion coefficient and high thermal conductivity. These properties are suitable for many structural parts and mechanical components. SAF 2507 has high impact strength and is not suitable for long-term storage. Temperatures above 570°F may weaken its toughness.

Application fields of 2507 duplex stainless steel:

S25073 (2507) stainless steel pipe is a steel that is resistant to local corrosion among duplex stainless steels, especially pitting corrosion, and has the characteristics of high strength, resistance to chloride stress corrosion, and weldability. It is very suitable for chemical, petroleum, petrochemical and power applications. Heat exchange equipment using river water, groundwater and seawater as cooling media in industry, as well as pulp and paper industry, seawater desalination, flue gas purification, heat exchangers, chemical tanker piping systems, seawater systems, etc.

Supporting welding materials: ER2594 welding wire, E2594 welding rod

Application areas: pulp and paper industry, seawater desalination, flue gas purification, heat exchangers, chemical tanker piping systems, seawater systems, etc.

 